Embodiment 1
[0043] A composite wear-resistant rubber liner, the rubber liner is formed by bonding a composite rubber plate on the surface and an elastic rubber plate on the lower layer. According to the weight ratio, the composite rubber plate is composed of 80 parts of isoprene rubber, 4 parts composite fiber, 3 parts of reinforcing agent, 2 parts of filler, 2 parts of vulcanizing agent and 1 part of composite resin, wherein the composite fiber is nylon fiber, acrylic fiber and carbon fiber in a ratio of 7:3:1 The weight ratio is mixed, the reinforcing agent is made of sepiolite wool, nano-zinc powder and ethyl orthosilicate in a weight ratio of 4:1:10, and the filler is nanocrystalline boehmite, ammonium fluoride, boric acid, Elemental silicon powder and magnesium borate whiskers are made in a ratio of 10:0.5:0.5:5:3; the composite resin is bisphenol F type epoxy resin, hydrogenated bisphenol A type epoxy resin, bisphenol S type ring Oxygen resin, modified nano silicon dioxide and modif...
Embodiment 2
[0069] A composite wear-resistant rubber liner, the rubber liner is formed by bonding a composite rubber plate on the surface and an elastic rubber plate on the lower layer. According to the weight ratio, the composite rubber plate is composed of 84 parts of isoprene rubber, 5 parts composite fiber, 4 parts of reinforcing agent, 3 parts of filler, 3 parts of vulcanizing agent and 2 parts of composite resin, wherein the composite fiber is nylon fiber, acrylic fiber and carbon fiber in a ratio of 8:4:1 The weight ratio is mixed, the reinforcing agent is made of sepiolite wool, nano-zinc powder and ethyl orthosilicate in a weight ratio of 5:2:15, and the filler is nanocrystalline boehmite, ammonium fluoride, boric acid, Elemental silicon powder and magnesium borate whiskers are made in a ratio of 12:0.5:0.5:6:4; the composite resin is bisphenol F type epoxy resin, hydrogenated bisphenol A type epoxy resin, bisphenol S type ring Oxygen resin, modified nano silicon dioxide and modi...
Embodiment 3
[0095] A composite wear-resistant rubber liner, the rubber liner is formed by bonding a composite rubber plate on the surface and an elastic rubber plate on the lower layer. According to the weight ratio, the composite rubber plate is composed of 82 parts of isoprene rubber, 4.5 parts composite fiber, 3.5 parts of reinforcing agent, 2.5 parts of filler, 2.5 parts of vulcanizing agent and 1.5 parts of composite resin, wherein the composite fiber is nylon fiber, acrylic fiber and carbon fiber at a ratio of 7.5:3.5:1 The weight ratio is mixed, the reinforcing agent is made of sepiolite wool, nano-zinc powder and ethyl orthosilicate at a weight ratio of 4.5:1.5:12.5, and the filler is nanocrystalline boehmite, ammonium fluoride, boric acid, Elemental silicon powder and magnesium borate whiskers are made in a ratio of 11:0.5:0.5:5.5:3.5; the composite resin is bisphenol F type epoxy resin, hydrogenated bisphenol A type epoxy resin, bisphenol S type ring Oxygen resin, modified nano ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com