A technology of breaking hammer and hammer head, which is applied in the direction of manufacturing tools, heat treatment equipment, furnace types, etc., can solve the problems of reducing the mechanical properties of steel-bonded hard alloys, the smoke has not been fully resolved, and the impact on the compactness of the structure, etc., to achieve a combination Better effect, less brittle fracture, improved mechanical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0025] A method for preparing a crushing hammer head of the present invention, the following steps are performed in sequence:
[0026] a. Mix hydroxyl iron powder, titanium carbide powder and graphite powder, wherein the mass of titanium carbide powder accounts for 20% to 40% of the total mass of raw materials, add absolute ethanol as a molding agent, and then mold it to make a strip-shaped strip Embryo;
[0027] b, sintering the obtained elongated strip blank in a vacuum furnace to obtain a titanium carbide steel-bonded hard alloy strip;
[0028] c. Use green sand as the shape of the hammer head, pour the smelted carbon steel liquid into the hammer head, and then insert and cast the titanium carbide steel-bonded hard alloy insert obtained in the above steps on the end of the hammer head;
[0029] d. Carry out shakeout cleaning and de-gating riser treatment;
[0030] e. Take it out after quenching in the muffle furnace, and finally perform water quenching.
[0031] As a pre...
Embodiment 1
[0035] Mix hydroxyl iron powder, titanium carbide powder and graphite powder, wherein the quality of titanium carbide powder accounts for 20% of the total mass of the raw materials, add the mixed raw materials to anhydrous ethanol and mold them into a shape with a thickness of 6mm and a length of 50mm. Strips with a width of 10mm, place the strip-shaped blanks in a vacuum of 5×10 -3 MPa, sintering temperature of 1400 ℃ in a vacuum furnace for 2 hours, and finally cast the sintered insert on the end of the hammer head made of carbon steel; The hammer head is heat treated in a muffle furnace at a temperature of 860°C for 50 minutes, and finally water quenched; after the impact toughness and hardness test of the prepared hammer head, the impact value is 18J / cm 2 , the hardness is 48HRC.
Embodiment 2
[0037] Mix hydroxyl iron powder, titanium carbide powder and graphite powder, wherein the mass of titanium carbide powder accounts for 30% of the total mass of the raw materials, add the mixed raw materials to anhydrous ethanol, and press them into a thickness of 6mm and a length of 50mm. Strips with a width of 10mm, the strip-shaped blanks are placed in a vacuum of 5×10 -3 MPa, sintering temperature of 1400 ℃ in a vacuum furnace for 2 hours, and finally cast the sintered inlay on the end of the hammer head made of carbon steel; The hammer head was heat treated in a muffle furnace at a temperature of 860°C for 50 minutes, and finally water quenched; after the impact toughness and hardness tests of the prepared hammer head, the impact value was 15J / cm 2 , the hardness is 57HRC.
PUM
Property | Measurement | Unit |
---|---|---|
width | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com