High-reliability mine cable
A reliable and mining technology, used in power cables, insulated cables, and power cables including electronic controls, etc., can solve the problems of poor mechanical and electrical performance, low corrosion and toxicity, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] Embodiment 1: as figure 1 As shown, the high-reliability mining cable includes a wire core, a filling layer 1 wrapping the wire core, and a 3M 8882 elastic insulating and waterproof resin coating 2 coated on the outside of the filling layer 1, which is wrapped around the 3M 8882 elastic insulating and waterproof resin coating. The Teflon tape outside the layer 2 is wrapped around the cladding layer 3, and the rubber inner sheath 4 wrapped outside the Teflon tape wrapping layer 3 is extruded; the steel wire armor layer 5 wrapped outside the rubber inner sheath 4 is extruded and wrapped in the The rubber outer sheath 6 outside the steel wire armor layer 5; the wire cores include three power wire cores and three control wire cores;
[0020] The power core is composed of a conductor 7 and an insulating sheath 8 of Korea Hushi Chemical HDPE 5305E high-density polyethylene (HDPE) extruded outside the conductor 7;
[0021] The control wire core is made of silver-plated soft r...
Embodiment 2
[0027] Embodiment 2: High-reliability mining cable, the structure is the same as Embodiment 1, the difference is that the rubber material used for the rubber outer sheath and the rubber inner sheath is made by the following steps:
[0028](1) Add 0.7 parts of phytic acid and 0.6 parts of 2-octylphenol polyoxyethylene ether (SOPE-7) to 20 parts of purified water, then add 2.5 parts of nano-sized yttrium aluminate with an average particle size of 40nm, and 4 parts of nano-boron nitride with a diameter of 600nm; stir with a magnetic stirrer for 5 minutes, and ultrasonically vibrate for 120 minutes at 85°C; then dry in an oven at 50°C for 5 hours;
[0029] (2) Calcining 4 parts of hexaethylene glycol monodecyl ether, 1.3 parts of LD-100P borate coupling agent of Yangzhou Lida Resin Co., Ltd., 12 parts of hydroxyapatite with an average particle size of 20um, and an average particle size of 10um 21 parts of kaolin powder, 27 parts of superfine barium sulfate powder with an average p...
PUM
Property | Measurement | Unit |
---|---|---|
tensile strength | aaaaa | aaaaa |
tensile strength | aaaaa | aaaaa |
tensile strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com