[0020] After mixing 20 mg of aprepitant and 10 mg of polyvinyl caprolactam-polyvinyl acetate-polyethylene glycol graft copolymer, add an appropriate amount of deionized water and grind in a P7 miniature planetary high-energy ball mill for 60 minutes (grinding for 15 minutes, intermittent 10 minutes, cycled 4 times), the aprepitant nanocrystal suspension was obtained, and the concentration of aprepitant was 0.5 mg / ml. The average particle size of the aprepitant nanocrystals was determined to be 280nm. Dissolve 200mg of soybean lecithin in an appropriate amount of absolute ethanol, add the above-mentioned aprepitant nanocrystal suspension to emulsify, freeze-dry to make aprepitant nanocrystal lipid microcapsules, and measure its average particle size to be 130 μm .
Embodiment 2
[0022] Disperse 50 mg of aprepitant and 18850 mg of poloxamer in an appropriate amount of deionized water, and use an M-110L high-pressure micro-fluidic nano-homogenizer to homogenize for 10 cycles under the pressure of 9000 PSI to obtain aprepitant nanocrystal suspension agent, the concentration of aprepitant is 0.5mg / ml. The average particle size of the aprepitant nanocrystals was determined to be 380nm. Dissolve 300mg soybean lecithin and 200mg lecithin in an appropriate amount of absolute ethanol, add the above-mentioned aprepitant nanocrystal suspension to emulsify, freeze-dry to make aprepitant nanocrystal lipid microcapsules, and measure the average The particle size is 150 μm.
Embodiment 3
[0024] Aprepitant 20mg and polyvinylpyrrolidone K2515mg were mixed evenly and pulverized by a high-speed airflow mill, and then dispersed in an appropriate amount of deionized water to obtain aprepitant nanocrystal suspension. The concentration of aprepitant was 1.0mg / ml. The average particle size of the aprepitant nanocrystals was determined to be 475nm. Dissolve 100mg soybean phospholipid and 50mg hydrogenated phospholipid in an appropriate amount of absolute ethanol, add the above-mentioned aprepitant nanocrystal suspension to emulsify, spray dry to make aprepitant nanocrystal lipid microcapsules, and measure the average The particle size is 420 μm.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com