A composite electroplating, V8C7 technology, applied in the direction of electrolytic coatings, coatings, etc., can solve the problems of fracture failure, localized adiabatic shear band single shear crack, etc., to achieve less energy consumption, high raw material utilization, plating solution The effect of simple ingredients
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] (1) Nano V 8 C 7 For the pretreatment of powder, first weigh 8 grams of nano V 8 C 7 powder, add 500ml of 15wt% hydrochloric acid solution, heat to 60°C in a water bath, stir for 30min, and V 8 C 7 Wash the powder twice with deionized water after filtration;
[0020] (2) First weigh 0.1 g of tartaric acid and 0.1 g of sodium dodecylbenzenesulfonate, add 1000 ml of deionized water, heat to 90°C in a water bath, and stir until tartaric acid and sodium dodecylbenzenesulfonate dissolved; then weigh 100 grams of nickel sulfate (NiSO 4 ·6H 2 O), 15 grams of nickel chloride (NiCl 2 ·6H 2 O), 50 grams of ferrous sulfate (FeSO 4 ·7H 2 O), 10 grams of ferrous chloride (FeCl 2 4H 2 O), 30 grams of sodium hypophosphite (NaH 2 PO 2 ·H 2 O), 3 grams of ascorbic acid, 20 grams of boric acid (H 3 BO 3 ) was added to the above solution, stirred at room temperature until dissolved; then added the cleaned V 8 C 7 The powder was continuously stirred for 2 hours, then 0.2...
Embodiment 2
[0022] (1) Nano V 8 C 7 For the pretreatment of powder, first weigh 10 grams of nanometer V 8 C 7 powder, add 500ml of 15wt% hydrochloric acid solution, heat to 60°C in a water bath, stir for 30min, and V 8 C 7 Wash the powder twice with deionized water after filtration;
[0023] (2) First weigh 0.1 g of tartaric acid and 0.1 g of sodium dodecylbenzenesulfonate, add 1000 ml of deionized water, heat to 90°C in a water bath, and stir until the sodium dodecylbenzenesulfonate is dissolved; Then weigh 80 grams of nickel sulfate (NiSO 4 ·6H 2 O), 10 grams of nickel chloride (NiCl 2 ·6H 2 O), 40 grams of ferrous sulfate (FeSO 4 ·7H 2 O), 15 grams of ferrous chloride (FeCl 2 4H 2 O), 35 grams of sodium hypophosphite (NaH 2 PO 2 ·H 2 O), 3 grams of ascorbic acid, 10 grams of boric acid (H 3 BO 3 ) was added to the above solution, stirred at room temperature until dissolved; then added the cleaned V 8 C 7 The powder was continuously stirred for 2 hours, then 0.2 g of ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com