Cefquinome transfer factor emulsion and preparation method thereof
A transfer factor and cefquinome technology, applied in the field of cefquinome transfer factor emulsion and its preparation, can solve complex and diverse problems, low income, high risk, etc., to improve antibody titer and uniformity, and reduce immune stress Response, mitigation of immunosuppressive effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0034] (1) Heat 600g of white oil for injection (density 0.925g / ml) to 120°C-150°C, then add 12g of aluminum stearate to dissolve, cool to room temperature, add 40g of Span-80 and 50g of cefquinome sulfate Powder, stir and disperse, place in a colloid mill at 2900r / min×3min to disperse evenly to obtain a uniform suspension mixture, then cool to 10-15°C as the oil phase;
[0035] (2) Add 10g Tween-80 to 300g transfer factor solution (polypeptide content: 1mg / ml), dissolve and cool to 10-15°C as the water phase;
[0036] (3) Put the oil phase and water phase in a colloid mill at a ratio of 3:1, emulsify at 2900r / min for 6 minutes, cool to room temperature, and emulsify again for 4 minutes to obtain a milky white to light yellow uniform emulsion (similar to the state of milk )product.
[0037] There is no delamination after the product has been placed for 12 months;
Embodiment 2
[0039] (1) Heat 600g of white oil for injection (density 0.925g / ml) to 120°C-150°C, then add 12g of aluminum stearate to dissolve, cool to room temperature, add 40g of Span-80 and 100g of cefquinome sulfate Powder, mix and disperse, place in a colloid mill at 2900r / min×3min to disperse evenly to obtain a uniform suspension mixture, then cool to 10-15°C as the oil phase;
[0040] (2) Add 10g Tween-80 to 300g transfer factor solution (polypeptide content: 1mg / ml), dissolve and cool to 10-15°C as the water phase;
[0041] (3) Put the oil phase and water phase in a colloid mill at a ratio of 3:1, emulsify at 2900r / min for 6 minutes, cool to room temperature, and emulsify again for 4 minutes to obtain a milky white to light yellow uniform emulsion (similar to the state of milk )product. There is no delamination after the product has been placed for 12 months;
Embodiment 3
[0043](1) Heat 600g of white oil for injection (density 0.925g / ml) to 120°C-150°C, then add 12g of aluminum stearate to dissolve, cool to room temperature, add 30g of Span-80 and 100g of cefquinome sulfate Powder, mix and disperse, place in a colloid mill at 2900r / min×3min to disperse evenly to obtain a uniform suspension mixture, then cool to 10-15°C as the oil phase;
[0044] (2) Add 10g Tween-80 to 300g transfer factor solution (polypeptide content: 1mg / ml), dissolve and cool to 10-15°C as the water phase;
[0045] (3) Put the oil phase and water phase in a colloid mill at a ratio of 3:1, emulsify at 2900r / min for 6 minutes, cool to room temperature, and emulsify again for 4 minutes to obtain a milky white to light yellow uniform emulsion (similar to the state of milk )product.
[0046] There is no delamination after the product has been placed for 6 months;
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com