Degradable polymer blood vessel stent drug-eluting containing anticoagulant choline phosphate composition
A technology for degrading polymers and drug coatings, applied in the field of medical devices, can solve the problems of carrier shedding, rough surface, strong hydrophobicity, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] Embodiment one: after 0.3g polylactic acid (PDLLA), polyethylene glycol and phosphorylcholine copolymer are dissolved in 10ml acetone, add 0.2g superoxide dismutase ( SOD) stirred, dissolved evenly and filtered, sprayed on the bottom layer of the parylene (Parylene) polymer film and covered with 0.1g cyclosporin A and 0.3g polylactic acid (PDLLA) and polyethylene glycol copolymer intermediate drug-coated 316L stainless steel stent surface, volatilize the solvent in nitrogen, and rotate the angle of the stent to repeat spraying several times to make it evenly coated on the surface of the stent, volatilize the solvent in nitrogen and then vacuum Dry at room temperature for 12 hours under conditions. Sterilized by ethylene oxide.
Embodiment 2
[0034] Example 2: After 0.2g of polylactic acid (PDLLA) and phosphorylcholine blend was dissolved in 10ml of acetonitrile, 0.5g of lycopene, 0.01g of coenzyme Q10 and 0.01g of vitamin E were added After stirring, dissolving evenly and filtering, spraying on the bottom layer of the polyparaxylylene (Parylene) polymer film is covered with 0.1g dactinomycin and 0.3g polylactic acid (PDLLA) and polyethylene glycol copolymer intermediate drug-coated 316L stainless steel stent surface, volatilize the solvent in nitrogen, and repeat the spraying several times by rotating the angle of the stent to make it evenly coated on the surface of the stent, volatilize the solvent in nitrogen, and then spray it under vacuum conditions. Dry at room temperature for 12 hours. Sterilized by ethylene oxide.
Embodiment 3
[0035] Example 3: After 0.3g of polylactic acid (PDLLA), polyethylene glycol and phosphorylcholine copolymer was dissolved in 10ml of ethanol, 0.3g of coenzyme Q10 and 0.01g of thunderbolt were added Pamycin was stirred, dissolved evenly and filtered, sprayed onto the surface of a 316L stainless steel stent covered with a bottom layer of a parylene (Parylene) polymer film, and rotated the angle of the stent to repeat spraying several times to make it evenly coated on the surface of the stent. The solvent was evaporated in nitrogen and then dried at room temperature under vacuum for 12 hours. Sterilized by ethylene oxide.
PUM
Property | Measurement | Unit |
---|---|---|
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com