Ergothioneine-lipid complex gel and preparation method therefor
The technology of lipid complex and ergothioneine is applied in the directions of pharmaceutical formulations, cosmetic preparations, cosmetic preparations, etc., and can solve the problems of damage of antioxidant properties, decreased activity and the like, and achieves simple preparation process, resistance to damage, and preparation of The effect of easy operation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] An ergothioneine lipid complex gel, prepared from the following raw materials in parts by weight: 1 part of ergothioneine, 8 parts of phospholipids, 0.2 parts of polyol esters, 10 parts of carbomer, 60 parts of glycerin, propylene glycol 10 parts, 5 parts of N-trimethyl chitosan, 0.1 part of Kathon.
[0026] The phospholipid is lecithin.
[0027] The polyol esters are mixed with 0.1 part of stearyl alcohol and 0.1 part of polyethylene glycol-12-hydroxystearate.
[0028] A preparation method for ergothioneine lipoplex gel, comprising the following steps:
[0029] 1) Weigh 1 part of ergothioneine, 8 parts of phospholipids, and 0.2 parts of polyol esters, add anhydrous ethanol to dissolve, heat and reflux at 50°C for 1 hour, leave at room temperature for 24h, use a rotary evaporator to evaporate in a 55°C water bath under reduced pressure Ethanol, vacuum drying at room temperature for 24 hours to obtain ergothioneine lipid complex;
[0030] 2) Take step (1) obtained erg...
Embodiment 2
[0033] An ergothioneine lipid complex gel, which is prepared from the following raw materials in parts by weight: 1 part of ergothioneine, 15 parts of phospholipids, 1 part of polyol esters, 15 parts of carbomer, 110 parts of glycerin, propylene glycol 30 parts, 12 parts of N-trimethyl chitosan, 0.15 parts of Kathon.
[0034] The phospholipid is soybean phospholipid.
[0035] The polyol esters are mixed with 0.5 part of stearyl alcohol and 0.5 part of polyethylene glycol-12-hydroxystearate.
[0036] A preparation method for ergothioneine lipoplex gel, comprising the following steps:
[0037] 1) Weigh 1 part of ergothioneine, 15 parts of phospholipids, and 1 part of polyol ester, add absolute ethanol to dissolve, heat and reflux at 50°C for 1 hour, leave at room temperature for 24h, use a rotary evaporator to evaporate in a water bath at 55°C under reduced pressure Ethanol, vacuum drying at room temperature for 24 hours to obtain ergothioneine lipid complex;
[0038] 2) Take...
Embodiment 3
[0041] An ergothioneine lipid complex gel, prepared from the following raw materials in parts by weight: 1 part of ergothioneine, 20 parts of phospholipids, 1.5 parts of polyol esters, 20 parts of carbomer, 150 parts of glycerin, propylene glycol 50 parts, 20 parts of N-trimethyl chitosan, 0.2 part of Kasong.
[0042] The phospholipid is hydrogenated soybean lecithin.
[0043] The polyol esters are mixed with 1 part of stearyl alcohol and 0.5 part of polyethylene glycol-12-hydroxystearate.
[0044] A preparation method for ergothioneine lipoplex gel, comprising the following steps:
[0045] 1) Weigh 1 part of ergothioneine, 20 parts of phospholipids, and 1.5 parts of polyol esters, add absolute ethanol to dissolve, heat and reflux at 50°C for 1 hour, leave at room temperature for 24h, use a rotary evaporator to evaporate in a 55°C water bath under reduced pressure Ethanol, vacuum drying at room temperature for 24 hours to obtain ergothioneine lipid complex;
[0046]2) Take ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.