A new dustproof, antibacterial and antiviral nanofiber mask
A nanofiber and anti-virus technology, applied in fiber treatment, fiber chemical characteristics, protective clothing, etc., can solve the problems of weak anti-virus and difficult storage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] A preparation method of a novel dustproof, antibacterial and antiviral nanofiber mask, comprising the following steps:
[0032] (1) The preparation method of ordinary non-woven fabric layer: in the form of melt blowing, the high-speed hot air flow drafts the thin stream of polyethylene melt extruded from the spinneret hole of the die head, and the formed fibers are collected on the drum, and at the same time Self-bonding to prepare melt-blown non-woven fabrics.
[0033] (2) The preparation method of drug-loaded nano-microspheres is as follows:
[0034] Dissolve cetyltrimethylammonium bromide surfactant in water, keep stirring at 60°C for 1 hour, add triethanolamine and ethyl orthosilicate in sequence, cetyltrimethylammonium bromide: triethanolamine: Ethyl orthosilicate: water = 0.4g: 0.3g: 6mL: 80mL, stirred and reacted and then centrifugally filtered, the obtained filter residue was dried at 80°C for 6h, and calcined in a muffle furnace at 300°C for 3h to obtain powde...
Embodiment 2
[0039] A preparation method of a novel dustproof, antibacterial and antiviral nanofiber mask, comprising the following steps:
[0040] (1) The preparation method of ordinary non-woven fabric layer: in the form of melt blowing, the high-speed hot air flow drafts the thin stream of polyacrylonitrile melt extruded from the spinneret hole of the die head, and the formed fibers are collected on the condensed net curtain , At the same time, it is self-adhesive to prepare a melt-blown non-woven fabric.
[0041] (2) The preparation method of drug-loaded nano-microspheres is as follows:
[0042] Dissolve sodium dodecylbenzenesulfonate surfactant in water, keep stirring at 80°C for 0.5h, add triethanolamine and ethyl orthosilicate in sequence, sodium dodecylbenzenesulfonate: triethanolamine: orthosilicate Ethyl ester: water = 1g: 0.8g: 10mL: 100mL, after stirring and reacting, centrifugal suction filtration, the resulting filter residue was dried at 80°C for 4h, and calcined at 400°C f...
Embodiment 3
[0048] A preparation method of a novel dustproof, antibacterial and antiviral nanofiber mask, comprising the following steps:
[0049] (1) The preparation method of ordinary non-woven fabric layer: in the form of melt blowing, the high-speed hot air flow drafts the thin stream of PVC melt extruded from the spinneret hole of the die head, and collects the formed polyvinyl chloride on the condensate screen fibers, and at the same time bond themselves to prepare melt-blown non-woven fabrics.
[0050] (2) The preparation method of drug-loaded nano-microspheres is as follows:
[0051] Dissolve sodium dodecylbenzenesulfonate surfactant in water, keep stirring at 80°C for 2 hours, add triethanolamine and ethyl orthosilicate in sequence, sodium dodecylbenzenesulfonate: triethanolamine: ethyl orthosilicate Ester: water = 1g: 0.8g: 10mL: 100mL, after stirring and reacting, centrifugal suction filtration, the resulting filter residue was dried at 80°C for 5h, and calcined at 450°C for 2...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com