A construction method and toilet technology, applied in building components, building insulation materials, etc., can solve the problems affecting the quality of lower building ceilings, bulging of the putty layer of the ceiling, easy-wear waterproof coating, etc., achieve good impervious and waterproof effects, and are easy to use Keeping dry and improving the effect of frost resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0081] A kind of cement mortar, refer to figure 2 , the preparation method of cement mortar is as follows:
[0082] S01. Add 100kg of Portland cement, 90kg of water, and 11kg of water reducing agent into the stirring tank at a rotating speed of 80r / min, and stir for 5min to form cement slurry;
[0083] S02. Add 35 kg of polyurethane adhesive and 3 kg of silane coupling agent to the cement slurry, at a rotating speed of 70 r / min, and stir for 5 min to form a premix;
[0084] S03. Add 100kg of nano fillers to the premix, rotate at a speed of 55r / min, and stir for 8min to form a mixture;
[0085] S04. Add 350kg of fine aggregate to the mixture, and stir at a speed of 45r / min for 10 minutes to form cement mortar, at a speed of 20r / min, and continue to stir until it is used up.
[0086] In the present embodiment, the nanofiller comprises the following components by mass ratio:
[0087] Nano granite powder: nano dolomite powder: nano basalt powder: nano limestone powder: nano wo...
Embodiment 2
[0089] A kind of cement mortar, refer to figure 2 , the preparation method of cement mortar is as follows:
[0090] S01. Add 100kg of Portland cement, 100kg of water, and 10kg of water reducing agent into the stirring tank at a speed of 80r / min, and stir for 5min to form cement slurry;
[0091] S02. Add 37.5kg of polyurethane adhesive and 4kg of silane coupling agent to the cement slurry, at a speed of 70r / min, and stir for 5min to form a premix;
[0092] S03. Add 110kg of nano fillers to the premix, rotate at a speed of 55r / min, and stir for 8min to form a mixture;
[0093] S04. Add 375kg of fine aggregate to the mixture, and stir at a speed of 45r / min for 10 minutes to form cement mortar, at a speed of 20r / min, and continue to stir until it is used up.
[0094] In the present embodiment, the nanofiller comprises the following components by mass ratio:
[0095] Nano granite powder: nano dolomite powder: nano basalt powder: nano limestone powder: nano wollastonite powder: ...
Embodiment 3
[0097] A kind of cement mortar, refer to figure 2 , the preparation method of cement mortar is as follows:
[0098] S01. Add 100kg of Portland cement, 110kg of water, and 9kg of water reducing agent into the stirring tank at a speed of 80r / min, and stir for 5min to form cement slurry;
[0099] S02. Add 40kg of polyurethane adhesive and 5kg of silane coupling agent to the cement slurry, rotate at 70r / min, and stir for 5min to form a premix;
[0100] S03. Add 120kg of nano fillers to the premix, rotate at a speed of 55r / min, and stir for 8min to form a mixture;
[0101] S04. Add 400kg of fine aggregate to the mixture, and stir at a speed of 45r / min for 10 minutes to form cement mortar, at a speed of 20r / min, and continue to stir until it is used up.
[0102] In the present embodiment, the nanofiller comprises the following components by mass ratio:
[0103] Nano granite powder: nano dolomite powder: nano basalt powder: nano limestone powder: nano wollastonite powder: nano zi...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com