[0020] (1) Preparation of modified ultraviolet absorber
[0021] Put 10g of 3,5-dihydroxy-6-(2,6-dihydroxyphenol)-1,2,4-triazine, 0.3g of kaolin, and 0.3g of talc into a ball mill, using ethanol as the medium, grind and mix thoroughly for 2h, Put it in a muffle furnace at 1000°C for 3 hours, then take it out as the furnace cools to obtain a modified UV absorber;
[0022] (2) The parts by weight of TPU coating are as follows: polyester thermoplastic polyurethane elastomer 50g, hexamethylene diisocyanate 6g, sodium carboxymethyl cellulose 12g, anatase nano titanium dioxide 6g, p-methoxy cinnamon 5 g of isooctyl acid, 8 g of modified UV absorber, 3 g of butyl reclaimed rubber, 3 g of paraffin oil, 0.5 g of zinc myristate, 5.5 g of butylene acetate, and 1 g of glycerol acetate. Through the laminating machine, pour 10g TPU coating liquid on both sides of 100g polyester filament mesh cloth.
Embodiment 2
[0024] (1) Preparation of modified ultraviolet absorber
[0025] Put 10g 3-mercapto-5,6-(2,6-dihydroxyphenol)-1,2,4-triazine, 0.2g kaolin, and 0.5g talc into a ball mill, using ethanol as the medium, grind and mix well for 2h, put Put it into the muffle furnace and keep it at 1000°C for 3 hours, then take it out as the furnace cools to get the modified UV absorber;
[0026] (2) The weight parts of TPU coating are as follows: polyether polyurethane elastomer 62g, isophorone diisocyanate 5g, sodium carboxymethyl cellulose 10g, anatase nano titanium dioxide 5g, p-methoxycinnamic acid 8 g of isooctyl ester, 3 g of modified UV absorber, 2 g of butyl reclaimed rubber, 2 g of paraffin oil, 0.5 g of zinc myristate, and 2.5 g of dipropyl carbonate. Through the laminating machine, pour 15g TPU coating liquid on both sides of 100g polyester filament mesh cloth.
Embodiment 3
[0028] (1) Preparation of modified ultraviolet absorber
[0029] Put 10g 3-mercapto-5,6-(2,6-dihydroxyphenol)-1,2,4-triazine, 0.2g kaolin, and 0.3g talc into a ball mill with ethanol as the medium, grind and mix well for 2h, put Put it into the muffle furnace and keep it at 1000°C for 3 hours, then take it out as the furnace cools to get the modified UV absorber;
[0030] (2) The parts by weight of the TPU coating are as follows: polyether polyurethane elastomer 55g, hexamethylene diisocyanate 4g, isophorone diisocyanate 5g, sodium carboxymethyl cellulose 10g, anatase nano titanium dioxide 5g, 5g isooctyl p-methoxycinnamate, 6g modified UV absorber, 2g butyl reclaimed rubber, 2g paraffin oil, 0.5g zinc myristate, 5.5g dipropyl carbonate. Pour 20g TPU coating solution on both sides of 100g polyester filament mesh cloth through the laminating machine.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
transmittivity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com