Preparation method of ozone heterogeneous oxidation solid catalyst
A heterogeneous oxidation, solid catalyst technology, applied in catalyst activation/preparation, physical/chemical process catalyst, metal/metal oxide/metal hydroxide catalyst, etc., can solve the problem of poor anti-toxicity, low catalyst adsorption, It is easy to lose catalytic activity and other problems, and achieve the effects of strong adsorption, inhibition of melting and precipitation, and improvement of anti-toxicity and catalytic activity.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0007] Embodiment 1:1.35g lithium hypochlorite, 1.65g bis(acetylacetonate) beryllium, 140ml deionized water, join volume and be that in the sealable reactor of 500ml, stir and mix evenly, the weight concentration of this aqueous solution is 2.1%, times Lithium chlorate: bis(acetylacetonate) beryllium weight ratio=1:1.2; add deionized water to wash to neutral, dry at 103°C to remove moisture, and then sieve 2.75g attapulgite of -200 mesh to +400 mesh standard sieve Weight of soil, 3.75g diopside, 4.75g bentonite, 5.75g polyhalite, 6.75g fly ash, 7.75g coal gangue, lithium hypochlorite and bis(acetylacetonate)beryllium (3g): weight of porous material (31.5g)=1:10.5, heat up to 36°C, continue to stir for 3.2h, filter, dry at 103°C and obtain 31g of pore-enlarging modified carrier; put 31g of pore-enlarging modified carrier into a 500ml ultrasonic reactor , then add 3.25g of trioctylmethylammonium chloride and dissolve in 100ml of deionized water. The weight concentration of the a...
Embodiment 2
[0008] Embodiment 2:0.24g lithium hypochlorite, 0.36g bis(acetylacetonate) beryllium, 10ml deionized water, join volume and be that in the sealable reactor of 100ml, stir and mix evenly, the weight concentration of this aqueous solution is 5.7%, times Lithium chlorate: the weight ratio of bis(acetylacetonate) beryllium=1:1.5; add deionized water to wash to neutral, dry at 103°C to remove moisture, and then sieve 1.45g attapulgite of -200 mesh to +400 mesh standard sieve Weight of soil, 1.65g diopside, 1.85g bentonite, 2.05g polyhalite, 2.25g fly ash, 2.45g coal gangue, lithium hypochlorite and bis(acetylacetonate) beryllium (0.6g): Porous material Weight (11.7g) = 1:19.5, heat up to 48°C, continue to stir for 5.8h, filter, dry at 105°C and obtain 11.5g of pore-enlarging modified carrier; in a 100ml ultrasonic reactor, put pore-enlarging modified Carrier 11.5g, then add 2.2g of trioctylmethylammonium chloride dissolved in 26ml of deionized water aqueous solution, the weight con...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com