A technology of heterogeneous oxidation and solid catalyst, applied in the direction of heterogeneous catalyst chemical elements, physical/chemical process catalysts, metal/metal oxide/metal hydroxide catalysts, etc., can solve the problem of low catalyst adsorption, anti-toxicity Poor, easy to lose catalytic activity and other problems, to achieve the effect of inhibiting precipitation, strong adsorption, improving anti-toxicity and catalytic activity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0007] Embodiment 1:1.4g lithium hypochlorite, 1.7g two (acetylacetonate) beryllium, 140ml deionized water, join volume and be that in the sealable reactor of 500ml, stir and mix evenly, the weight concentration of this aqueous solution is 2.2%, times Lithium chlorate: the weight ratio of bis(acetylacetonate) beryllium=1:1.2; add deionized water to wash to neutral, dry at 103°C to remove moisture, and then sieve 2.8g erionite of -200 mesh to +400 mesh standard sieve , 3.8g garnet, 4.7g medical stone, 5.8g wollastonite, 6.7g activated carbon, 7.8g carnallite, weight of lithium hypochlorite and bis(acetylacetonate) beryllium (3.1g): weight of porous material (31.6g)=1:10.2, heat up to 36°C, continue to stir and react for 3.2h, filter, dry at 103°C and obtain 30g of pore-enlarging modified carrier; put 30g of pore-enlarging modified carrier into a 1L ultrasonic reactor , then add 3.3g dodecyltrimethylammonium chloride dissolved in 100ml deionized water aqueous solution, the weigh...
Embodiment 2
[0008] Embodiment 2:0.24g lithium hypochlorite, 0.36g bis(acetylacetonate) beryllium, 10ml deionized water, join volume and be that in the sealable reactor of 100ml, stir and mix evenly, the weight concentration of this aqueous solution is 5.7%, times Lithium chlorate: the weight ratio of bis(acetylacetonate) beryllium=1:1.5; add deionized water to wash to neutral, dry at 103°C to remove moisture, and then sieve 1.45g erionite of -200 mesh to +400 mesh standard sieve , 1.65g garnet, 1.85g medical stone, 2.05g wollastonite, 2.25g activated carbon, 2.45g carnallite, weight of lithium hypochlorite and bis(acetylacetonate) beryllium (0.6g): weight of porous material (11.7g)=1:19.5, heat up to 48°C, continue to stir for 5.8h, filter, dry at 105°C and obtain 11.5g of pore-enlarging modified carrier; in a 100ml ultrasonic reactor, put the pore-enlarging modified carrier 11.5g, then add 2.2g dodecyltrimethylammonium chloride and be dissolved in the aqueous solution of 26ml deionized w...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com