Method for making bricks from coal slime based on high-sulfur coal gangue
A technology for high-sulfur coal gangue and coal gangue particles, which is used in solid separation, clay products, other household appliances, etc. Great, reduce the effect of environmental pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] The invention provides a method for making bricks based on high-sulfur coal gangue sorting coal slime, and the specific steps are as follows:
[0029] Step 1, ore grinding: first crush and grind the high-sulfur coal gangue to obtain coal gangue particles, and the particle size of the coal gangue particles is 170 mesh;
[0030] Step 2, mixing slurry: adding water to the gangue particles to prepare a primary slurry, the mass concentration of the primary slurry is 25%, and adding water to the gangue particles and stirring for 10 to 15 minutes;
[0031] Step 3, cyclone separation: the ore slurry is separated through a cyclone separator. Specifically, a hydrocyclone is used, the cone angle of the hydrocyclone is 18°, the cone ratio is 0.50, the cyclone separation pressure is 0.16 MPa, and the cyclone separation time is 3 to 5 minutes;
[0032] Step 4, primary concentration treatment: the upper light material obtained by the cyclone separation is placed in the first stirring...
Embodiment 2
[0039] Step 1, ore grinding: first crush and grind the high-sulfur coal gangue to obtain coal gangue particles, and the particle size of the coal gangue particles is 200 mesh;
[0040] Step 2, mixing slurry: adding water to the gangue particles to prepare a primary slurry, the mass concentration of the primary slurry is 20%, and adding water to the gangue particles and stirring for 10-15 minutes;
[0041] Step 3, cyclone separation: the ore slurry is separated through a cyclone separator. Specifically, a hydrocyclone is used, the cone angle of the hydrocyclone is 18°, the cone ratio is 0.50, the cyclone separation pressure is 0.16 MPa, and the cyclone separation time is 3 to 5 minutes;
[0042] Step 4, primary concentration treatment: the upper light material obtained by the cyclone separation is placed in the first stirring tank, and water is added to prepare a secondary pulp, the mass concentration of the secondary pulp is 50%; then, it is treated by stirring and centrifugal...
Embodiment 3
[0049] Step 1, ore grinding: first crush and grind the high-sulfur coal gangue to obtain coal gangue particles, and the particle size of the coal gangue particles is 230 mesh;
[0050] Step 2, mixing slurry: adding water to the gangue particles to prepare a primary slurry, the mass concentration of the primary slurry is 15%, and adding water to the coal gangue particles and stirring for 10-15 minutes;
[0051] Step 3, cyclone separation: the ore slurry is separated through a cyclone separator. Specifically, a hydrocyclone is used, the cone angle of the hydrocyclone is 16°, the cone ratio is 0.50, the cyclone separation pressure is 0.16 MPa, and the cyclone separation time is 3 to 5 minutes;
[0052] Step 4, primary concentration treatment: the upper light material obtained by the cyclone separation is placed in the first stirring tank, and water is added to prepare a secondary pulp, the mass concentration of the secondary pulp is 40%; then, it is treated by stirring and centri...
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com