Embodiment 1
[0027] This embodiment provides a water-resistant colloidal emulsion explosive, and the components are proportioned according to the following parts by mass:
[0028] 88 parts of ammonium nitrate
[0029] Sodium nitrate 10 parts
[0030] Potassium nitrate 4 parts
[0031] urea 5 parts
[0032] 1 part emulsifier
[0033] 11 parts of water
[0034] Oil phase 5 parts
[0035] 6 parts expanded perlite
[0036] Mixed rare earth 0.5 parts.
[0037] Among them, the emulsifier includes: 4 parts of polyisobutenyl succinimide, 15 parts of polyglycerin fatty acid ester, 15 parts of lecithin, 55 parts of sorbitan monooleate; the oil phase includes: 22 parts of paraffin, 8 parts of silicone oil, 12 parts of Vaseline, 4 parts of polystyrene, and 3 parts of polypropylene; mixed rare earths include: 8% cerium, 15% neodymium, 13% gadolinium, 17% erbium, and the rest is lanthanum.
[0038] This embodiment also provides a method for preparing a water-resistant colloidal emulsion explosiv...
Embodiment 2
[0045] This embodiment provides a water-resistant colloidal emulsion explosive, and the components are proportioned according to the following parts by mass:
[0046] Ammonium nitrate 96 parts
[0047] Sodium nitrate 6 parts
[0048] Potassium nitrate 8 parts
[0049] 3 parts urea
[0050] 3 parts emulsifier
[0051] 9 parts water
[0052] Oil phase 7 parts
[0053] 4 parts expanded perlite
[0054] Mixed rare earth 1.5 parts.
[0055] Among them, the emulsifier includes: 6 parts of polyisobutenyl succinimide, 5 parts of polyglycerin fatty acid ester, 22 parts of lecithin, 45 parts of sorbitan monooleate; the oil phase includes: 28 parts of paraffin, 6 parts of silicone oil, 14 parts of Vaseline, 2 parts of polystyrene, and 5 parts of polypropylene; mixed rare earths include: 11% cerium, 12% neodymium, 16% gadolinium, 15% erbium, and the rest is lanthanum.
[0056] This embodiment also provides a method for preparing a water-resistant colloidal emulsion explosive, comp...
Embodiment 3
[0063] This embodiment provides a water-resistant colloidal emulsion explosive, and the components are proportioned according to the following parts by mass:
[0064] Ammonium nitrate 92 parts
[0065] Sodium nitrate 8 parts
[0066] Potassium nitrate 6 parts
[0067] 4 parts urea
[0068] 2 parts emulsifier
[0069] 10 parts of water
[0070] Oil phase 6 parts
[0071] 5 parts expanded perlite
[0072] Mixed rare earth 1 part.
[0073] Among them, the emulsifier includes: 5 parts of polyisobutenyl succinimide, 10 parts of polyglycerin fatty acid ester, 18 parts of lecithin, 50 parts of sorbitan monooleate; the oil phase includes: 25 parts of paraffin, 7 parts of silicone oil, 13 parts of Vaseline, 3 parts of polystyrene, and 4 parts of polypropylene; mixed rare earths include: 10% cerium, 13% neodymium, 15% gadolinium, 16% erbium, and the rest is lanthanum.
[0074] This embodiment also provides a method for preparing a water-resistant colloidal emulsion explosive, co...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com