A starch adhesive, bio-oil technology, applied in the direction of adhesives, grafted polymer adhesives, adhesive types, etc., can solve the problems of poor process stability, increased adhesive costs, and high adhesive costs, and achieve good environmental coordination Excellent environmental protection performance and low total volatile organic compounds

Active Publication Date: 2013-05-29
BEIJING FORESTRY UNIVERSITY +1
View PDF7 Cites 18 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] The starch used in the first step of the preparation method is mechanically activated starch, which needs to be invested in special starch processing equipment, which will lead to an increase in the cost of the adhesive; in the third and fourth steps of the preparation of the adhesive, glyoxal and emulsion copolymerization, oxalic acid on the starch During esterification, the addition of glyoxal, oxalic acid, sodium hydroxide, etc. will cause pH fluctuations and temperature rises in the reaction system. In these cases, if the process parameters are not adjusted in time, the emulsion will quickly gel and agglomerate, and the process is stable. In the fifth step of the preparation of the adhesive, in order to ensure the water resistance and wet bonding strength of the adhesive, so that its bonding performance is equivalent to that of urea-formaldehyde resin, it is necessary to add a high-priced curing agent isocyanate in the glue mixing process, which reduces the cost of the adhesive. high

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

preparation example Construction

[0020] The preparation method of the bio-oil starch adhesive that the present invention proposes comprises the following steps:

[0021] The first step: prepare 80-120 parts of starch with 150 parts of 0.3-0.6mol / L hydrochloric acid to prepare a starch emulsion with a mass fraction of 40%, and raise the temperature to 45-55°C within 10 minutes and maintain the temperature until the third step , add 2-5 parts of oxidizing agent, carry out acid hydrolysis oxidative denaturation for 30-60min, obtain acid hydrolysis oxidative denaturation starch emulsion;

[0022] The second step: add 1-3 parts of emulsifier and 10-20 parts of stabilizer with a mass fraction of 10% to the acid-hydrolyzed oxidized modified starch emulsion, and adjust the pH value to within 10 minutes with sodium hydroxide with a mass fraction of 10%. 4-5, add 10-20 parts of acrylamide in 3-6 batches within 30-60 minutes, continue to react for 30-60 minutes, add 0.3-0.6 parts of initiator and react for 30-60 minutes...

Embodiment 1

[0026] The mass parts of each raw material component of the present embodiment are as follows: 80 parts of tapioca starch, 150 parts of hydrochloric acid, 2 parts of ammonium persulfate oxidant, 1 part of sodium lauryl sulfate emulsifier, 10 parts of polyvinyl alcohol stabilizer, ammonium persulfate trigger 0.3 parts of agent, 10 parts of acrylamide, 5 parts of bio-oil, 5 parts of glyoxal crosslinking agent, 10 parts of flour filler;

[0027] The preparation method of the bio-oil starch adhesive of the present embodiment may further comprise the steps:

[0028] Step 1: Prepare 80 parts of cassava starch with 150 parts of 0.3mol / L hydrochloric acid to make a starch emulsion with a mass fraction of 40%, and raise the temperature to 45°C within 10 minutes and keep this temperature until the third step, adding 2 parts of mass The fraction is 10% ammonium persulfate solution, which is subjected to acid hydrolysis and oxidative denaturation for 30 minutes to obtain acid hydrolysis a...

Embodiment 2

[0033] The mass parts of each raw material component in this embodiment are as follows: 100 parts of cornstarch, 150 parts of hydrochloric acid, 3 parts of potassium persulfate oxidizing agent, 2 parts of sodium dodecylbenzenesulfonate emulsifier, 15 parts of polyvinyl alcohol stabilizer, persulfate 0.4 parts of potassium initiator, 15 parts of acrylamide, 10 parts of bio-oil, 7.5 parts of glutaraldehyde crosslinking agent, 15 parts of light calcium carbonate filler;

[0034] The preparation method of bio-oil starch adhesive comprises the following steps:

[0035] Step 1: Prepare 100 parts of cornstarch with 150 parts of 0.4mol / L hydrochloric acid to make a starch emulsion with a mass fraction of 40%, and raise the temperature to 50°C within 10 minutes and keep the temperature until the third step, adding 3 parts of mass Fraction is 10% potassium persulfate solution, carry out acid hydrolysis oxidative denaturation 45min, obtain acid hydrolysis oxidative denaturation starch em...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
Shear strengthaaaaaaaaaa
Shear strengthaaaaaaaaaa
Login to View More

Abstract

The invention relates to a bio-oil starch adhesive for wood, which belongs to the technical field of adhesive preparation. A preparation method comprises the following steps: carrying out acidolysis, oxidation and denaturation on starches by using a hydrochloric acid and an oxidant so as to reduce the molecular weight of the starches and improve the reactivity of the starches; then, adding an emulsifier and a stabilizer into the obtained object, and carrying out graft copolymerization on the obtained mixture and acrylamide under the action of an initiator; adding bio-oil, so that chemical groups on a skeleton structure are modified by using substances such as acid and aldehyde and the like in the bio-oil, thereby obtaining a host adhesive; and finally, adding a crosslinking agent and packing into the host adhesive so as to obtain the bio-oil starch adhesive, wherein the mass part of each raw material component is as follows: 80-120 parts of the starches, 150 parts of the hydrochloric acid, 2-5 parts of the oxidant, 1-3 parts of the emulsifier, 10-20 parts of the stabilizer, 0.3-0.6 part of the initiator, 10-20 parts of the acrylamide, 5-20 parts of the bio-oil, 5-10 parts of the crosslinking agent, and 10-15 parts of the packing. The bio-oil starch adhesive disclosed by the invention can replace a white emulsion and can be widely used in the aspects of wood ornaments, wood processing and artificial boards.

Description

technical field [0001] The invention belongs to the technical field of adhesive preparation, in particular to a method for preparing a bio-oil starch adhesive for wood. Background technique [0002] As a kind of natural adhesive, starch adhesive has the advantages of light weight, no corrosion, no pollution, easy to obtain raw materials, low price, and convenient use. It is widely used for bonding paper, cotton fabrics, trademarks, etc. However, starch adhesives have disadvantages such as low bonding strength and easy mildew when exposed to moisture, which limits the application in the bonding of wood products. In the patent CN201210135823.6, the applicant provides a starch-based adhesive prepared in five steps using bio-oil, mechanically activated starch, glyoxal, oxalic acid, water, oxidant, curing agent polyisocyanate, filler, etc. as raw materials Methods. Firstly, mechanically activated starch is used to prepare starch emulsion, and then it is subjected to acid hydrol...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C09J151/02C09J11/06C08F251/00C08F220/56C08F8/00C08B31/18
Inventor 常建民张琪张继宗王大张冯绍园许守强
Owner BEIJING FORESTRY UNIVERSITY
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products