Macromolecule waterproof coating capable of being subjected to microwave heating and preparation method thereof
A technology of polymer waterproofing and microwave heating, applied in radiation-absorbing coatings, asphalt coatings, recycled rubber coatings, etc. Impact resistance, good elasticity and flexibility, the effect of improving waterproof reliability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0044] The ratio of each component of the raw material of the polymer waterproof coating that can be heated by microwave in the present invention is as follows:
[0045] Thermoplastic polyolefin (TPO) 10%
[0046] Bitumen 45%
[0047] Conductive polymer polyaniline 1.5%
[0048] Waste vulcanized rubber powder 20%
[0049] Magnetic metal powder 2.5%
[0050] Maleic anhydride 1%
[0051] Talc 17%
[0052] Tetrahydrofuran 3%.
[0053] The preparation method of the above-mentioned microwave-heatable polymer waterproof coating is as follows:
[0054] 1) Add polyolefin thermoplastic (TPO) and polyaniline to tetrahydrofuran to swell and soften;
[0055] 2) Add 20% of the total amount of asphalt and maleic anhydride, heat to 200°C, stir for 60-120 minutes, and enter the colloid mill for 30 minutes;
[0056] 3) Then add the remaining asphalt, waste vulcanized rubber powder, magnetic metal powder, talcum powder, etc., stir and mix at 150°C for 60 minutes, then put it into the mo...
Embodiment 2
[0064] The ratio of each component of the raw material of the polymer waterproof coating that can be heated by microwave in the present invention is as follows:
[0065] Styrenic thermoplastic elastomer (SBS) 25%
[0066] Bitumen 35%
[0067] Polypyrrole 1.5%
[0068] Waste vulcanized rubber 17%
[0069] Ferrite 2.5%
[0070] N-Methylpyrrolidone 1%
[0071] Activated Calcium Carbonate 13%
[0072] Xylene 5%.
[0073] The preparation method of the above-mentioned microwave-heatable polymer waterproof coating is as follows:
[0074] 1) Add styrene-based thermoplastic elastomer (SBS) and polypyrrole to xylene to swell and soften;
[0075] 2) Add 20% of the total amount of asphalt and N-methylpyrrolidone, heat to 200°C, stir for 60-120 minutes, and enter the colloid mill for 30 minutes;
[0076] 3) Add the remaining asphalt, waste vulcanized rubber powder, ferrite, and activated calcium carbonate, stir and mix at 150°C for 60 minutes, then put it into the mold, cool down a...
PUM
Property | Measurement | Unit |
---|---|---|
tensile strength | aaaaa | aaaaa |
tensile strength | aaaaa | aaaaa |
tensile strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com