A fireproof insulation board and inorganic technology, applied in the field of building materials, can solve the problems of failing to meet the A-level requirements, large thermal conductivity, limited use range, etc., to achieve good economic and social benefits, excellent fire performance, and expanded use. range effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Raw material ratio: The ratio is based on the solid content of water glass glue. The solid content of water glass glue is 50%. Aluminum oxide accounts for 3% of the solid content of water glass glue, zinc oxide accounts for 5%, calcium carbonate accounts for 40%, fly ash accounts for 36%, magnesium oxide accounts for 20%, magnesium chloride accounts for 22%, starch accounts for 2%, waterproof agent ( Organosilicon waterproofing agent, produced by Jinan Guobang Chemical Co., Ltd.) accounted for 3%. The weight ratio of polyphenylene particles to water glass glue (based on its solid content, the same below) is 1:1.
[0022] Production process: Mix and stir the above-mentioned inorganic raw materials, then mix and stir with polystyrene particles, shape through the production line, microwave (or light wave, or high-temperature drying room) at 120°C-200°C, dry at high temperature, and demould, and you can get Inorganic modified polystyrene particle fireproof insulation boar...
Embodiment 2
[0024] Raw material ratio: The ratio is based on the solid content of water glass glue. The solid content of water glass glue is 40%. Aluminum oxide accounts for 6% of the solid content of water glass glue, zinc oxide accounts for 3%, calcium carbonate accounts for 30%, fly ash accounts for 30%, magnesium oxide accounts for 15%, magnesium chloride accounts for 25%, starch accounts for 3%, waterproofing agent ( Silicone waterproofing agent) accounted for 1.5%. The weight ratio of polyphenylene particles to water glass glue is 1:1.
[0025] Production process: Mix and stir the above-mentioned inorganic raw materials, then mix and stir with polystyrene particles, shape through the production line, microwave (or light wave, or high-temperature drying room) at 120°C-200°C, dry at high temperature, and demould, and you can get Inorganic modified polystyrene particle fireproof insulation board.
Embodiment 3
[0027] Raw material ratio: The ratio is based on the solid content of water glass glue. The solid content of water glass glue is 80%. Aluminum oxide accounts for 9% of the solid content of water glass glue, zinc oxide accounts for 7%, calcium carbonate accounts for 50%, fly ash accounts for 30%, magnesium oxide accounts for 15%, magnesium chloride accounts for 28%, starch accounts for 7%, waterproofing agent ( Stearic acid waterproofing agent, produced by Hunan Tongyun Building Materials Technology Co., Ltd.) accounted for 6%. The weight ratio of extruded particles to water glass glue is 1:1.
[0028] Production process: Mix and stir the above-mentioned inorganic raw materials, then mix and stir with polystyrene particles, shape through the production line, microwave (or light wave, or high-temperature drying room) at 120°C-200°C, dry at high temperature, and demould, and you can get Inorganic modified polystyrene particle fireproof insulation board.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com