Wound-protection liquid, and its preparing method
A technology of silver ion powder and pure water, which is applied in the field of wound care liquid, can solve the problems of harsh processing conditions, irritating smell, and lack of permeability, etc., and achieve the effects of shortening healing time, no side effects, and shortening the treatment cycle
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A) Add 0.18g of superfine silver ion powder produced and sold by commercially available, such as Shenzhen Zhiyuan Kejia Technology Co., Ltd., Guangdong Province, China, to 10g of silver ion powder, and the purity measured by the conductivity meter is 0.1- Stir evenly in 0.16μs / cm deionized water, and the container used can be either a polyethylene plastic container or a stainless steel container, until the silver ion powder is fully dissolved, thereby obtaining the silver ion powder liquid;
[0026] B) the phosphoric acid of 0.52g reagent grade is joined in the silver ion powder body liquid obtained by A) step and carry out acidification treatment, the time of acidification treatment is 30min, adjust PH2, obtain the silver ion powder body mixed solution after acidification treatment;
[0027] C) adding 0.42 g of reagent-grade tartaric acid obtained commercially, such as produced and sold by China Shanghai Reagent No. 1 Factory, into 10 g of deionized water with the same ...
Embodiment 2
[0033] A) Add 0.22 g of superfine silver ion powder produced and sold by commercially available, such as Shenzhen Zhiyuan Kejia Technology Co., Ltd., Guangdong Province, China, to 10 g of silver ion powder, and the purity measured by the conductivity meter is 0.1- Stir evenly in distilled water of 0.16μs / cm, the container used can be either a polyethylene plastic container or a stainless steel container, until the silver ion powder is fully dissolved, so as to obtain the silver ion powder body liquid;
[0034] B) 0.66g of reagent-grade phosphoric acid is added to the silver ion powder liquid obtained in step A) to carry out acidification treatment, the time of acidification treatment is 18min, and the pH is adjusted to 1.8 to obtain the silver ion powder mixed solution after acidification treatment ;
[0035] C) adding 0.50 g of reagent-grade tartaric acid obtained commercially, such as produced and sold by China Shanghai Reagent No. 1 Factory, into 10 g of distilled water wit...
Embodiment 3
[0040]A) Add 0.30 g of superfine silver ion powder, such as produced and sold by Shenzhen Zhiyuan Kejia Technology Co., Ltd., Shenzhen City, Guangdong Province, into 10 g of commercially available and the purity measured by the conductivity meter is 0.1- Stir evenly in 0.16μs / cm deionized water, and the container used can be either a polyethylene plastic container or a stainless steel container, until the silver ion powder is fully dissolved, thereby obtaining the silver ion powder liquid;
[0041] B) Add 0.74g of reagent-grade citric acid to the silver ion powder liquid obtained in step A) to carry out acidification treatment, the time of acidification treatment is 35min, adjust the pH to 1.5, and obtain the mixed silver ion powder after the acidification treatment liquid;
[0042] C) adding 0.66 g of reagent-grade tartaric acid obtained commercially, such as produced and sold by China Shanghai Reagent No. 1 Factory, into 10 g of deionized water with the same purity of 0.1-0....
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com