A technology of non-woven fabrics and silk, which is applied in the fields of non-woven fabrics, textiles, papermaking, medical science, etc., can solve the problems of silk easy to dissolve and stick, waste water pollutes the environment, has no health care and nutritional effects, and achieves good economic benefits and reduces Environmental pollution, soft touch effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Weigh 10 kg silkworm cocoon silk, remove impurities, put it into the refining pool and soak it fully with clean water, pick it up and dry it in the drying room, set the temperature at 80°C, and dry it; then soak it again, and then dry it. Repeat 2 times. Then put it into 0.5% Turkish red oil solution and soak until soft, take it out, put it into a normal temperature alkaline solution with PH=8.5 and hydrogen peroxide content of 1% and soak for 10 hours, turn it once an hour, wash after soaking, dehydrate, and dry. Dry at 70°C; then, comb the dried cocoon silk with a carding machine, and shorten it into short fiber filaments with an average length of 3 cm; use the obtained short fiber cocoon silk as the raw material of the spunlace production line, Adjust the baking temperature in the spunlace process to 70°C for carding, web laying, and spunlace production to obtain silk denatured non-woven fabrics rich in sericin. The obtained silk denatured non-woven fabric is used a...
Embodiment 2
[0023] Weigh 15 kg of castor silk, remove impurities, put it into the refining pool and soak it fully with clean water, pick it up and dry it in the drying room, set the temperature at 100 ° C, and dry it; then soak it again, dry it again, repeat Do this 4 times. Then put in 2% softener KC or softener SCM or softener NDS or softener SD or softener DMD solution to soak until soft, take it out, put it into a normal temperature alkaline solution with PH=8.5 and hydrogen peroxide content of 2%. 12 hours, turning once an hour, washing after soaking, dehydration, and drying at 80°C; then, combing the dried cocoon silk with a carding machine, and shortening it into short fibers with an average length of 3 cm; The obtained short fibrous cocoon silk is used as the raw material of the spunlace production line, and the baking temperature in the spunlace process is adjusted to 80°C for carding, web laying, and spunlace production to obtain silk denatured non-woven fabrics rich in sericin ...
Embodiment 3
[0025] Weigh 8 kg of cocoon silk, remove impurities, put it into the refining pool and soak for 2 hours, the sulfuric acid solution in the pool is PH=2, 98 kg, dehydrate after soaking; put the dehydrated cocoon silk into the glutaraldehyde solution for soaking After 10 hours, this solution can also be formaldehyde or monoaldehyde solution, the concentration is 2%, the sulfuric acid is adjusted to PH=2, and dehydration is carried out after soaking; the cocoon silk after dehydration is put into PH=10 again, the hydrogen peroxide content is 1% Soak in alkaline solution for 10 hours, wash after soaking (bleaching), dehydrate, and dry at a temperature of 40°C to 80°C; comb and shorten the dried cocoon silk with a carding machine to an average length of 4 cm In the form of short fibers, adjust the baking temperature in the spunlace process to 50°C for carding, laying, and spunlace production to obtain silk denatured non-woven fabrics rich in sericin. The obtained silk denatured non-...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com