Beneficiation inhibitor and purification method of molybdenum rough concentrate
A purification method and inhibitor technology, applied in flotation, solid separation, etc., can solve the problems of application limitation, phosphoknox is highly toxic, etc., achieve strong inhibition, reduce impurity content, and reduce the pressure of subsequent lead reduction Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] The raw material is a molybdenum rough concentrate in Heilongjiang, which contains 10.25% molybdenum, 5.12% copper, and 2.13% lead. It also contains a certain amount of pyrite and gangues such as quartz, chalcedony and mica. Coarse concentrate weight is 100 grams.
[0031] The inhibitor is prepared from thioglycolic acid, sodium silicate and glucuronic acid as raw materials, and the weight ratio of the three is 40:500:1. Dissolve the three in water according to this ratio to make an aqueous solution with a weight concentration of 5%.
[0032] Such as figure 1 As shown, the present embodiment provides a method for purifying molybdenum rough concentrate, which specifically includes the following steps:
[0033] (1) Gravity separation: Use a fine-grained shaking table to carry out shaking table gravity separation of molybdenum coarse concentrate to obtain gravity separation concentrate and gravity separation tailings products mainly composed of lead impurities; The shak...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com