A technology of chemical sensors and composite thin films, applied in the direction of electrochemical variables of materials, scientific instruments, instruments, etc., can solve problems such as difficult exposure, difficult transfer of electrons, poor chemical stability and thermal stability of enzyme molecules, etc., and achieve electrochemical signal Improvement, rapid electrocatalytic performance, good response effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] 1. The preparation mass fraction is the naphthol green solution A of 1g / L;
[0020] 2. Preparation of nitrate hydrotalcite by ion exchange method:
[0021] a. Dissolve 0.01mol of solid Co(NO3)2·6H2O and 0.005mol of solid Al(NO3)3·9H2O and 0.06mol of urea in 50mL of deionized water in a 90 ml polytetrafluoroethylene pressure reaction vessel , crystallized at 120°C for 48 hours, centrifuged with deionized water until the pH was about 7, and dried at 50°C for 24 hours to obtain carbonate intercalated hydrotalcite powder;
[0022] b. Dissolve 0.3g of the above-mentioned carbonate intercalated hydrotalcite powder and 363.75g of solid NaNO3 in 300mL of deionized water without CO2. After uniform dispersion, add 0.09mL of concentrated nitric acid and stir at 20°C under a nitrogen atmosphere to perform ionization. After 24 hours of exchange reaction, it was centrifuged and washed with deionized hot water without CO2 until the pH was about 7, and vacuum dried at 50°C for 24 hour...
Embodiment 2
[0028] 1. The preparation mass fraction is the naphthol green solution A of 1g / L;
[0029] 2. With embodiment 1;
[0030] 3. Obtain clear transparent colloidal solution B with embodiment 1;;
[0031] 3. Grind the glassy carbon electrode sheet into a mirror surface with 0.05 μm Al2O3 powder, wash it with ultrapure water, and ultrasonically in concentrated nitric acid, absolute ethanol, and ultrapure water for 30 seconds, and put the cleaned glassy carbon electrode sheet in the solution Soak in A for 10 minutes, fully wash with deionized water, place in solution B, soak for 10 minutes and fully wash to obtain a cycle of naphthol green and hydrotalcite composite film;
[0032] 4. repeat step 3, 12 times, obtain naphthol green and hydrotalcite multilayer composite film, get hydrogen peroxide electrochemical sensor after vacuum drying.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com