A fire-proof board and board technology, which is applied in the direction of floors, coverings/linings, buildings, etc., can solve the problems that the filling is difficult to continuously resist flame burning, the alloy has low fire resistance, and the fire prevention effect is not good, etc., to achieve excellent fire resistance and fire resistance , good sealing and tight structure
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036] Prepare the skeleton: select high-quality pine wood, dry it and process it into a standard material, place the standard material in a vacuum environment, control the vacuum degree to be less than 0.01Pa, and evenly spread a layer of magnesium hydroxide and silicon dioxide on the standard material mixed powder, the amount of mixed powder is 130kg / m 3 , and then slowly apply the pressure to 70MPa, keep it for 5h, then carry out secondary drying, and assemble it into a fireproof board skeleton after trimming.
[0037] Calcium carbide substrate preparation: the calcium carbide substrate is selected according to its composition and parts by weight. Raw materials: 110 parts of CaO, 100 parts of kaolinite, 25 parts of mullite fiber, Fe 2 o 3 4 parts, polyvinyl alcohol 15 parts, dolomite fiber 40 parts, water 700 parts. The specific preparation process is as follows: first mix and grind CaO, iron oxide and some kaolinite, add appropriate amount of water to form an emulsion, u...
Embodiment 2
[0041] Prepare the skeleton: select high-quality pine wood, dry it and process it into a standard material, place the standard material in a vacuum environment, control the vacuum degree to be less than 0.01Pa, and evenly spread a layer of magnesium hydroxide and silicon dioxide on the standard material mixed powder, the amount of mixed powder is 120kg / m 3 , and then slowly apply the pressure to 60MPa, keep it for 3 hours and then carry out secondary drying, and assemble it into a fireproof board skeleton after trimming.
[0042] Calcium carbide substrate preparation: the calcium carbide substrate is selected according to its composition and parts by weight. Raw materials: 110 parts of CaO, 100 parts of kaolinite, 25 parts of mullite fiber, Fe 2 o 3 4 parts, polyvinyl alcohol 15 parts, dolomite fiber 40 parts, water 700 parts. The specific preparation process is as follows: first mix and grind CaO, iron oxide and some kaolinite, add appropriate amount of water to form an emu...
Embodiment 3
[0046] Prepare the skeleton: select high-quality pine wood, dry it and process it into a standard material, place the standard material in a vacuum environment, control the vacuum degree to be less than 0.01Pa, and evenly spread a layer of magnesium hydroxide and silicon dioxide on the standard material mixed powder, the amount of mixed powder is 140kg / m 3 , and then slowly apply the pressure to 80MPa, keep it for 7 hours, then carry out secondary drying, and assemble it into a fireproof board skeleton after trimming.
[0047] Calcium carbide substrate preparation: the calcium carbide substrate is selected according to its composition and parts by weight. Raw materials: 110 parts of CaO, 100 parts of kaolinite, 25 parts of mullite fiber, Fe 2 o 3 4 parts, polyvinyl alcohol 15 parts, dolomite fiber 40 parts, water 700 parts. The specific preparation process is as follows: first mix and grind CaO, iron oxide and some kaolinite, add appropriate amount of water to form an emulsi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com