A preparation method of long afterglow nanocrystals controlled by emission wavelength
A technology with emission wavelength and long afterglow, applied in nanotechnology, nano-optics, nanotechnology and other directions, it can solve the problems of requiring special equipment and high risks, and achieve the effects of controllable emission wavelength, low cost and simple operation.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] A method for preparing long afterglow nanocrystals controlled by emission wavelength, which is prepared by ethylene glycol-assisted hydrothermal method, and the steps are as follows:
[0025] 1) Preparation of gallium nitrate solution: reflux gallium oxide solid and 1:3 nitric acid solution at 100° C. until gallium oxide is completely dissolved, so that the concentration of the solution is 0.20 mol / liter.
[0026] 2) Preparation of indium trichloride solution: Stir the indium trichloride solid and deionized water until the indium trichloride is completely dissolved, so that the concentration of the solution is 0.20 mol / liter.
[0027] 3) Preparation of chromium nitrate solution: Stir the chromium nitrate solid and deionized water until the chromium nitrate is completely dissolved, so that the concentration of the solution is 0.01 mol / liter.
[0028] 4) Mix ethylene glycol, the gallium nitrate solution obtained in step 1), the indium trichloride solution obtained in step...
Embodiment 2
[0036] A method for preparing long-lasting nanocrystals regulated by emission wavelength, which is prepared by ethylene glycol-assisted hydrothermal method. The steps and methods are basically the same as those in Example 1, except that:
[0037] The reflux temperature in step 1) is 90°C;
[0038] In step 4), the mass ratio of gallium nitrate aqueous solution and indium trichloride aqueous solution in the mixed solution was changed to 55.78:1.53:0.575:0.016; the mixed solution was obtained by stirring at a temperature of 18°C for 30 minutes, and then the mass percentage concentration was 15%. ammonia water to adjust the pH of the mixed solution to 7.0, and continue to stir at a temperature of 18° C. for 1 hour to obtain a mixed solution;
[0039] Step 5) The temperature of the reactor is set to 190° C., and the hydrothermal treatment is carried out for 20 hours;
[0040] Step 6) centrifuge rotation speed is 8000rpm;
[0041] Step 7) drying in a vacuum oven at a temperature...
Embodiment 3
[0045] A method for preparing long-lasting nanocrystals regulated by emission wavelength, which is prepared by ethylene glycol-assisted hydrothermal method. The steps and methods are basically the same as those in Example 1, except that the pH of the mixed solution is changed to 8 in step 4). .
[0046] The long afterglow luminescent nanocrystal prepared in this example was taken as the observation afterglow and characterization sample, and the test results were similar to those in Example 1.
PUM
![No PUM](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/noPUMSmall.5c5f49c7.png)
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com