Drag reducer and preparation method and application thereof
A technology of drag reducer and emulsifier, which is applied in the field of drag reducer and its preparation, and drag reducer, which can solve the problems of crude oil displacement and high interfacial tension of drag reducer, so as to reduce the flow resistance of crude oil and reduce the oil-water interface Tension, raw materials can be selected from a wide range of effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] 1. Preparation of high molecular weight polymer
[0031] Mix 3.5 parts by weight of an emulsifier composed of Tween-80 and nonylphenol polyoxyethylene ether with 45 parts by weight of solvent oil composed of cyclohexane and white oil to make an oil phase solvent, wherein Tween-80 and nonyl The mass ratio of phenol polyoxyethylene ether is 4:5, and the mass ratio of cyclohexane to white oil is 4:1. After stirring for 20 minutes, add 7 parts by weight of lipophilic acrylic monomer composed of ethyl methacrylate and methoxy polyethylene glycol methacrylate to the oil phase solvent, wherein ethyl methacrylate and methoxy The mass ratio of the base polyethylene glycol methacrylate was 1.5:1, and the mixture was kept stirring for 30 minutes to obtain an oil phase mixed solution.
[0032] Add 20 parts by weight of a hydrophilic monomer composed of dimethylacrylamide and methacrylic acid to 42 parts by weight of water, wherein the mass ratio of dimethylacrylamide to methacryli...
Embodiment 2
[0040] 1. Preparation of high molecular weight polymer
[0041] 4 parts by weight of an emulsifier composed of Tween-40 and dodecylphenol polyoxyethylene ether are mixed with 47 parts by weight of solvent oil composed of xylene and kerosene to make an oil phase solvent, wherein Tween-40 and dodecylphenol The mass ratio of alkylphenol polyoxyethylene ether is 2:5, and the mass ratio of xylene to kerosene is 1:3. After stirring for 10 min, add 8.5 parts by weight of lipophilic acrylic monomers composed of ethyl acrylate and stearyl acrylate to the oil phase solvent, wherein the mass ratio of ethyl acrylate to stearyl acrylate is 1.5:4, keeping Stir for 25 min to obtain a mixed solution of oil phase.
[0042] Add 27 parts by weight of a hydrophilic monomer composed of methylolacrylamide and acrylic acid to 45 parts by weight of water, wherein the mass ratio of methylolacrylamide to acrylic acid is 1:1. After stirring for 10 min, the pH value of the solution was adjusted to 8 wi...
Embodiment 3
[0050] 1. Preparation of high molecular weight polymer
[0051] Mix 5 parts by weight of an emulsifier composed of Tween-20 and dinonylphenol polyoxyethylene ether with 45 parts by weight of solvent oil composed of toluene and cyclopentane to make an oil phase solvent, wherein Tween-20 and dinonylphenol The mass ratio of phenol polyoxyethylene ether is 1:1, and the mass ratio of cyclopentane to toluene is 2:1. After stirring for 15 minutes, add 5 parts by weight of lipophilic acrylic monomers composed of butyl acrylate and hexyl acrylate to the oil phase solvent, wherein the mass ratio of butyl acrylate to hexyl acrylate is 2:1, and keep stirring for 20 minutes , to obtain an oil phase mixed solution.
[0052] Add 28 parts by weight of a hydrophilic monomer composed of dimethylacrylamide, acrylic acid and acrylamide to 50 parts by weight of water, wherein the mass ratio of methacrylamide, acrylic acid and acrylamide is 2:1:1. After stirring for 20 min, the pH value of the so...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com