A cleaning material and machine screw technology, which is applied to chemical instruments and methods, detergent compositions, soap detergent compositions, etc., can solve the problems of inability to clean the hot runner of the screw and barrel, corrosion of cross-linked pipes, and large damage to equipment and other problems, to achieve rapid penetration and efficient cleaning effect, high mold release, and reduce procurement costs
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] A preparation method for a cleaning material for a novel extruder screw, comprising the following steps:
[0027] Step 1: High Speed Mixing
[0028] Get 60Kg linear low density polyethylene LLDPE powder, 20Kg low density polyethylene resin LDPE, 8Kg diethylene glycol butyl ether, 3Kg carbon tetrachloride, 3Kg polyethylene glycol 400, 5Kg ethanolamine, 2KgEBS, 3Kg methyl vinyl silicone oil , 5Kg calcium stearate, 2Kg 10# white oil, 5Kg polyethylene wax, 20Kg talcum powder are added in the high-speed mixer, and mixed at room temperature for 3-5 minutes.
[0029] Step Two: Mixing
[0030] Put the mixed materials in the first step into the banbury mixer for banburying, the banburying temperature is 90-100°C, and the banburying time is 6-8 minutes.
[0031] Step 3: Granulation
[0032] Put the materials mixed in the second step into the parallel twin-screw extrusion granulator for extrusion and granulation. The working temperature of the extruder is set as: 110±5℃ in th...
Embodiment 2
[0034] A preparation method for a cleaning material for a novel extruder screw, comprising the following steps:
[0035] With embodiment 1, difference is: the first step: get 80Kg linear low density polyethylene LLDPE powder, 40Kg low density polyethylene resin LDPE, 10Kg diethylene glycol butyl ether, 5Kg carbon tetrachloride, 5Kg polyethylene glycol Alcohol 400, 8Kg ethanolamine, 3KgEBS, 5Kg methyl vinyl silicone oil, 8Kg calcium stearate, 3Kg 10# white oil, 8Kg polyethylene wax, 30Kg talcum powder.
Embodiment 3
[0037] A preparation method for a cleaning material for a novel extruder screw, comprising the following steps:
[0038] With embodiment 1, difference is: the first step: get 70Kg linear low density polyethylene LLDPE powder, 30Kg low density polyethylene resin LDPE, 9Kg diethylene glycol butyl ether, 4Kg carbon tetrachloride, 4Kg polyethylene glycol 400, 7Kg ethanolamine, 2.5Kg EBS, 4Kg methyl vinyl silicone oil, 7Kg calcium stearate, 2.5Kg 10# white oil, 7Kg polyethylene wax, 25Kg talcum powder.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com