Toner, image forming method, image forming apparatus, and process cartridge
A technology of toner and colorant, applied in the field of toner, which can solve the problems of easily damaged toner capsule structure and poor fusion, and achieve the effect of stabilizing developability and improving chargeability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0083] "Masterbatch preparation method"
[0084] The masterbatch may be prepared by mixing / kneading the colorant for the masterbatch with the resin by applying high shear force. Also, organic solvents may be used to improve mixing between these materials. In addition, it is preferable to use a flash evaporation method in which an aqueous paste containing a colorant is mixed / kneaded with a resin and an organic solvent, and then the colorant is transferred to the resin to remove water and the organic solvent, because the Wet cake (ie, without drying) of the colorant described above. In such mixing / kneading, it is preferable to use a high-shear disperser (such as a three-roll mill).
[0085]
[0086] The external additive is not particularly limited, and inorganic particles and polymer particles known in the art can be preferably used. The primary particle size of the external additive is preferably 5 nm to 2 μm, more preferably 5 nm to 500 nm. The specific surface area det...
Embodiment 1
[0346]
[0347] Ion-exchanged water (963 parts), organic resin particles (copolymer of styrene-methacrylic acid-butyl acrylate-methacrylic acid ethylene oxide adduct sodium salt of sulfuric acid ester) for stable dispersion 88 parts of a 25% aqueous dispersion, 80 parts of a 48.5% aqueous solution of sodium dodecyl diphenyl ether disulfonate (Eleminol MON-7, a product of Sanyo Chemical Industries Ltd.), and 113 parts of ethyl acetate were mixed under stirring together to obtain a milky liquid. This liquid is referred to as aqueous phase 1.
[0348]
[0349] Polyester 1 (378 parts), paraffin ((HNP9, product of NIPPON SEIRO CO., Ltd.) (120 parts) and ethyl acetate (1450 parts) were charged into a container in which a stirring bar and a thermometer had been set. The The mixture was warmed to 80° C. with stirring, held at 80° C. for 5 hours, and cooled to 30° C. over 1 hour. The vessel was then charged with masterbatch 1 (500 parts) and ethyl acetate (500 parts), After that,...
Embodiment 2
[0365] Toner 2 of Example 2 was obtained in the same manner as in Example 1 except that the resin dispersion liquid 1 in the protrusion forming step was changed to the resin dispersion liquid 2 .
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
acid value | aaaaa | aaaaa |
acid value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com