Composite fuel-saving device and coating
A paint and fuel economizer technology, applied in the direction of charging system, coating, mechanical equipment, etc., can solve the problems of efficiency drop, thermal, magnetic, electrical and other physical properties discount, decomposition and damage, etc., to avoid damage.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] Embodiment 1: A composite fuel-saving device, including but not limited to fuel tank, fuel pipe, water tank, water pipe, air intake pipe or fuel economizer, fuel-saving ball, fuel block or air filter placed in the fuel tank Filter equipment or anti-scale equipment placed in the water tank.
[0029] The composite fuel-saving device is formed by mixing tourmaline powder and plastic powder with a weight ratio of 1:1-1:10 through injection molding machine. The weight ratio of tourmaline in the molded composite fuel-saving device is greater than or equal to 3%. In order to make the tourmaline evenly distributed in the composite fuel-saving device after injection molding, it can be injected multiple times.
[0030] The plastic powder includes one or a combination of polyethylene, polypropylene, polyvinyl chloride, and ABS plastic. The powder diameter of tourmaline powder is 450-550nm. The infrared normal emissivity of tourmaline powder near this diameter range reaches the highest...
Embodiment 2
[0033] Example 2: A composite fuel-saving paint, which is formed by mixing tourmaline powder and plastic powder with a weight ratio of 1:1-1:30 and then adding them to the paint to uniformly mix. The weight ratio of tourmaline in the composite fuel-saving paint is greater than or equal to 3%.
[0034] The plastic powder includes one or a combination of polyethylene, polypropylene, polyvinyl chloride, and ABS plastic. The powder diameter of tourmaline powder is 450-550nm, and the tourmaline powder is magnesium tourmaline powder or lithium tourmaline powder or iron tourmaline powder.
[0035] In order to improve the fuel-saving function, a variety of synergists can be added to the formulation of the composite fuel-saving coating, such as ① rare earth-based catalysts with a weight ratio of 1%-2%, which include cerium, zirconium, lanthanum and cobalt; ② The weight ratio is 1%-5% of the magnetic material, the magnetic material includes neodymium iron boron; ③1-5mg / L metal oxide mixture...
PUM
Property | Measurement | Unit |
---|---|---|
Diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com