A technology of engine coolant and sodium tetraborate, which is applied in the direction of heat exchange materials, chemical instruments and methods, etc., can solve problems such as anti-corrosion protection of magnesium alloy engines, and achieve the goal of inhibiting gel precipitation and ensuring anti-corrosion performance Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] The formula of this embodiment: ethylene glycol 100kg, deionized water 90kg, sodium benzoate 1.3kg, sodium tetraborate decahydrate 1.2kg, sodium nitrate 0.1kg, terephthalic acid 0.7kg, sodium metasilicate pentahydrate 0.3kg, Silicate stabilizer (aqueous solution containing silicon hydroxyalkyl phosphate) 0.04kg, methyl benzotriazole 0.2kg, sodium hydroxide 0.2kg, defoamer (PE6400) 0.02kg, rhodamine B 0.01kg.
[0025] The blending process of the cooling liquid of the present invention is: according to the above weight, first mix deionized water and ethylene glycol at room temperature, then add sodium benzoate, sodium tetraborate, sodium nitrate, phthalic acid, sodium hydroxide, triazole, After all dissolved, add silicate stabilizer, stir evenly, then add sodium silicate, continue stirring to make it fully dissolved, finally add defoamer and dyeing agent, stir evenly, filter to get the finished product.
Embodiment 2
[0027] The formula of this embodiment: ethylene glycol 100kg, deionized water 60kg, sodium benzoate 1.0kg, sodium tetraborate decahydrate 1.0kg, sodium nitrate 0.5kg, phthalic acid 0.9kg, sodium metasilicate pentahydrate 0.4kg, Silicate stabilizer 0.03kg, sodium salt of methyl benzotriazole 0.1kg, sodium hydroxide 0.35kg, defoamer 0.03kg, rhodamine B 0.02kg. The blending process is the same as in Example 1.
Embodiment 3
[0029] The formula of the present embodiment: ethylene glycol 100kg, deionized water 160kg, sodium benzoate 1.6kg, sodium tetraborate pentahydrate 1.4kg, sodium nitrate 0.2kg, terephthalic acid 0.5kg, sodium metasilicate nonahydrate 0.5kg, Silicate stabilizer 0.05kg, benzotriazole 0.3kg, sodium hydroxide 0.3kg, defoamer (PE6400) 0.04kg, rhodamine B 0.015kg. The blending process is the same as in Example 1.
PUM
Property | Measurement | Unit |
---|---|---|
hardness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com