A montmorillonite gel agent and the technology of montmorillonite, which are applied in the field of medicine, can solve the problems of high viscosity, difficult to divide the dose accurately, poor taste, increase production cost, etc., and achieve fine particle size, reduce production cost and good effect. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Montmorillonite suspension formula:
[0022] Montmorillonite 300g Glucose 74.9g Sodium Saccharin 0.7g
[0023] Vanillin 0.4g Sodium Benzoate 9 Deionized Water 15000g
[0024] Preparation:
[0025] (1) Weigh the raw materials and auxiliary materials of the formula formula.
[0026] (2) Add montmorillonite into deionized water and stir evenly, then add sucrose and sodium benzoate, and stir evenly.
[0027] (3) Process the uniformly stirred mixed solution with a colloid mill to form a uniform suspension with a fineness of montmorillonite particles less than 10 μm.
[0028] (4) Suspension through cobalt 60 After irradiation sterilization, it can be obtained by dispensing.
Embodiment 2
[0030] Montmorillonite suspension formula:
[0031] Montmorillonite 200g, sucrose 150g, ethylparaben 0.5g,
[0032] Propylparaben 0.5g, deionized water 13000g.
[0033] Preparation:
[0034] (1) Weigh the raw materials and auxiliary materials of the formula formula.
[0035] (2) First add montmorillonite into deionized water and stir evenly, then add sucrose, glucose, ethylparaben and propylparaben and stir evenly.
[0036] (3) The homogeneously stirred mixed solution is then ultrasonically treated to form a uniform suspension with a particle size of montmorillonite less than 10 μm.
[0037] (4) After the suspension is boiled for 15 minutes to sterilize, it can be packaged separately.
Embodiment 3
[0039] Montmorillonite suspension formula:
[0040] Montmorillonite 250g, Aspartame 0.7g, Vanillin 0.3g,
[0041] Ethylparaben 5g, sodium benzoate 45g, deionized water 17000g.
[0042] Preparation:
[0043] (1) Weigh the raw materials and auxiliary materials of the formula formula.
[0044] (2) First add montmorillonite into deionized water and stir evenly, then add sucrose, glucose, ethylparaben and sodium benzoate and stir evenly.
[0045] (3) Process the uniformly stirred mixed solution with a homogenizer to form a uniform suspension with a fineness of montmorillonite particles less than 10 μm.
[0046] (4) The suspension was heated at 70°C for 1 hour, then placed at room temperature for 24 hours, and then heated at 70°C for 1 hour, and the heating and placing operations were continuously sterilized for 3-5 times.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com