Method for preparing long fiber reinforced ABS composite material
A composite material and long glass fiber technology, which is applied in the preparation of long glass fiber reinforced ABS composite materials by suspension impregnation method, and the preparation of high performance long glass fiber reinforced thermoplastic composite materials, which can solve the cumbersome process, high energy consumption and long time consumption and other problems, to achieve the effect of reducing the process, low energy consumption, and reducing the degree of damage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] Refer to attached figure 1 , mix the intermediate butadiene graft emulsion of ABS with SAN resin powder, the weight ratio of the dry weight of butadiene to SAN is 1:1.5, add ABS antioxidant 1010 to the mixture, stir at high speed, and obtain a uniform suspension; place the continuous glass fiber bundle at 400°C for 6 hours at high temperature, cool it down to room temperature naturally, then soak it in 1.5% silane coupling agent KH-550 aqueous solution for 20 minutes, and place it in an 80°C drying oven Medium drying; continuous glass fiber passes through the suspension infiltration tank under traction, is dried in an open oven, heated and melted through a closed melting pipeline, and then extruded through a mold, and pelletized to obtain a composite material slice; the composite material slice is Vacuum drying at 80°C for 4 hours, injection molding with an injection molding machine, to obtain long glass fiber reinforced ABS composite material.
Embodiment 2
[0028] Refer to attached figure 1 , mix the intermediate butadiene graft emulsion of ABS with SAN resin powder, the weight ratio of the dry weight of butadiene to SAN is 1:3, add ABS antioxidant 1010 to the mixture, stir at high speed, and obtain a uniform suspension; place the continuous glass fiber bundle at 450°C for 4 hours at high temperature, cool it down to room temperature naturally, then soak it in 1.5% silane coupling agent KH-550 aqueous solution for 15 minutes, and then place it in a 90°C drying oven Medium drying for 2 hours; continuous glass fiber passes through the suspension infiltration tank under the action of traction, is dried in an open oven, heated and melted through a closed melting pipeline, and then extruded through a mold, and pelletized to obtain composite material slices; composite material The slices were dried at 70°C for 5 hours under a vacuum degree of 0.1 MPa, and injected into an injection molding machine to obtain a long glass fiber reinforce...
Embodiment 3
[0030] Refer to attached figure 1 , mix the intermediate butadiene graft emulsion of ABS and SAN resin powder, the weight ratio of the dry weight of butadiene to SAN is 1:2.5, add ABS antioxidant 1010 to the mixture, stir at high speed, and obtain a uniform suspension; place the continuous glass fiber bundle at 500°C for 4 hours at high temperature, cool it down to room temperature naturally, then soak it in 1.5% silane coupling agent KH-550 aqueous solution for 30 minutes, and then place it in a 70°C drying oven Medium drying; continuous glass fiber passes through the suspension infiltration tank under traction, is dried in an open oven, heated and melted through a closed melting pipeline, and then extruded through a mold, and pelletized to obtain a composite material slice; the composite material slice is Vacuum drying at 90°C for 3 hours, and injection molding by an injection molding machine to obtain long glass fiber reinforced ABS composite materials.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
degree of grafting | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com