An air-purifying and stable technology, applied to polyester coatings, polyurea/polyurethane coatings, coatings, etc., can solve the problems of inability to guarantee long-term and stable release of negative ions, damage the stability of base materials, and short service life, and achieve a fresh environment Air, delicate touch, not easy to crack
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
example 1
[0043] Nano anion powder slurry formula 1 is as follows:
[0044] Tourmaline powder 50g
[0045] volcanic rock powder 20g
[0046] Maifan stone powder 20g
[0047] Propylene Glycol 10g
[0048] water 25 grams
[0049] Titanate dispersant 1.5g
[0050] Modified polyacrylate dispersant 1 g
[0051] 22 grams of water-based alkyd resin
[0052] Thickener 0.5g
[0053] In a 250ml dispersing kettle, first add 10 grams of propylene glycol, 2.5 grams of dispersant and 25 grams of water, stir evenly at a low speed, then add 90 grams of negative ion powder, disperse by ball milling for 2 hours, then ultrasonically disperse for 20 minutes, add 22 grams of water-based alkyd resin 1. Disperse 0.5 g of thickener at a low speed of 500 rpm for 10 minutes to prepare a stable nano-anion powder slurry 1 that can release negative ions automatically for a long time.
[0054] The formula 1 of long-lasting and stable air-purifying paint is as follows:
[0055] Nano negative ion powder slurr...
example 2
[0065] Nano-anion powder slurry formula 2 is as follows:
[0066] Titanium dioxide powder 30g
[0067] Jade powder 20g
[0068] Ceramic powder 25g
[0069] water 44 grams
[0070] Titanate dispersant 1 g
[0071] Polyacrylate alcohol amine salt dispersant 2 grams
[0072] Polyacrylic acid sodium salt dispersant 3 grams
[0073] Dispersant 6 grams
[0074] 20 grams of water-based polyurethane resin
[0075] Water-based amino resin 2 grams
[0076] Thickener 3 grams
[0077] In a 250ml dispersing kettle, first add 6 grams of dispersant and 44 grams of water, stir evenly at a low speed, then add 75 grams of negative ion powder, disperse by ball milling for 5 hours, then ultrasonically disperse for 10 minutes, add 20 grams of water-based polyurethane resin, 2 grams of water-based amino Resin and 3 grams of thickener were dispersed at a low speed of 1000rpm for 20 minutes to prepare a stable nano-anion powder slurry 2 that can release negative ions automatically for a long...
example 3
[0090] Nano anion powder slurry formula 3 is as follows:
[0091] Titanium dioxide powder 70g
[0092] Zeolite 30g
[0093] Ethylene glycol 4 grams
[0094] Ethylene glycol butyl ether 5 g
[0095] 30 grams of water
[0096] Fatty amine dispersant 4g
[0097] Titanate dispersant 1 g
[0098] Silicone-acrylate emulsion 5g
[0099] Thickener 1 g
[0100] In a 250ml dispersing kettle, first add 4 grams of ethylene glycol, 5 grams of ethylene glycol butyl ether, 5 grams of dispersant and 30 grams of water, stir evenly at a low speed, then add 100 grams of negative ion powder, disperse by ball milling for 5 hours, and then ultrasonically disperse After 60 minutes, add 5 grams of silicone-acrylate emulsion and 1 gram of thickener and disperse at a low speed of 1000 rpm for 20 minutes to prepare a stable nano-anion powder slurry 3 that can automatically release anions for a long time.
[0101] Long-term stable air purification paint formula 3 is as follows:
[0102] Nano neg...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com