Catalyst for improving organic sulfur hydrolysis rate, its carrier and preparation method
A technology of catalyst and hydrolysis rate, which is used in the purification of gas by catalytic conversion of impurities, chemical instruments and methods, catalysts for physical/chemical processes, etc. problem, to achieve the effect of improving low-temperature activity, increasing surface alkalinity, and enhancing surface alkalinity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0046] Take KNO 3 50 grams, dissolved in 200 ml of water, added 800 grams of aluminum hydroxide, 30 grams of metatitanic acid, kneaded, dried and roasted at 600 ° C for 3 hours, crushed to 180 mesh, and the alkaline material was obtained for use.
[0047] Take 20 grams of alkaline material, add 1000 grams of pseudo-boehmite, 200 grams of MgO, and 50 grams of scallop powder, mix well, knead and extrude with 30 grams of 10% nitric acid solution, and roast at 500 ° C for 3 hours to prepare the carrier.
[0048] Get 50 grams of carrier, 6 grams of ammonium molybdate, 3.0 grams of cobalt nitrate and 16 grams of potassium carbonate, and use 18% ammonia water to form a co-immersion solution, impregnate the carrier with equal volume of the solution and roast at 400 ° C to obtain a catalyst, wherein cobalt Calculated as CoO, it is 1.0% of the total amount of catalyst, molybdenum is calculated as MoO 3 Calculated as 4.8% of the total amount of catalyst, potassium is expressed as K 2...
Embodiment 2
[0051] MgSO 4 80g, dissolved in 200ml water, add r-AL 2 o 3 800 grams were kneaded, dried and roasted at 800°C for 2.5 hours, crushed to 180 meshes, and the alkaline material was obtained for use.
[0052] Take 100 grams of alkaline material, then add 1000 grams of gibbsite, 200 grams of CaO, and 40 grams of scallop powder, mix well, knead with 10 grams of 10% nitric acid solution, extrude and roast at 500 ° C for 3 hours Prepare the carrier.
[0053] Take 50 grams of carrier, 10 grams of ammonium molybdate, 1 gram of cobalt nitrate and 10 grams of potassium carbonate, and use 29 grams of 18% ammonia water to form a co-immersion solution, impregnate the carrier with equal volume of the solution and roast at 400 ° C to obtain a catalyst , where cobalt is 0.8% of the total amount of the catalyst as CoO, molybdenum as MoO 3 Calculated as 9% of the total amount of catalyst, potassium is expressed as K 2 O is counted as 5% of the total amount of catalyst.
[0054] The prepa...
Embodiment 3
[0056] The preparation method is the same as in Example 1, and the difference is that KNO 3 50 grams replaced by Ca(NO 3 ) 2 40 grams, the numbering of catalyst is SJB-3, and its performance comparison is as shown in table 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com