A desulfurization agent and flue gas technology, applied in the field of flue gas desulfurization agent and its preparation, can solve the problems of harsh temperature application range, low utilization rate of desulfurization agent, poor mechanical strength, etc., and achieve wide use temperature range and better desulfurization performance , Improve the effect of mechanical strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0049] In one embodiment of the present invention, a method for preparing the above-mentioned flue gas desulfurizer is provided, comprising the following steps:
[0050] (1) Calcium hydroxide is treated with surfactant, and modified calcium hydroxide is obtained after drying and pulverization;
[0051] (2) Mix modified calcium hydroxide, calcium carbonate and additives, stir to obtain mixed powder;
[0052] (3) Mix the mixed powder with the binder, stir evenly, add an appropriate amount of aqueous solution to fully knead, and obtain a kneaded solid;
[0053] (4) Extrude and shape the kneaded solid to obtain a molded product; dry the molded product to obtain a medium-low temperature high-performance desulfurizer.
[0054] In a specific implementation manner, the specific operation of step (1) is:
[0055] Weigh calcium hydroxide, add surfactant and appropriate amount of water, stir on a magnetic or mechanical stirrer, heat and steam until paste, then dry in an oven at 120°C and...
Embodiment 1
[0064] Preparation of modified calcium hydroxide:
[0065] Weigh 500g of calcium hydroxide passing through a 200-mesh sieve, add 30g of surfactant and an appropriate amount of water, stir on a magnetic or mechanical stirrer, heat and steam to a paste, then dry in an oven at 120°C and grind into powder to obtain Modified calcium hydroxide.
Embodiment 2
[0067] Preparation of desulfurizer:
[0068] Fully mix 200g of modified calcium hydroxide, 100g of calcium carbonate, 58g of sodium carbonate, and 40g of iron oxide, and stir evenly to obtain a mixed powder; after dry mixing and stirring, add 30g of bentonite, add an appropriate amount of water to the obtained dry powder, and fully Knead, then extrude, shape, and dry at 120°C for 3 hours to obtain the finished product A1 of medium and low temperature high-performance desulfurizer.
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Strength | aaaaa | aaaaa |
Specific surface area | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com