Production process of parts for oil exploitation equipment fracturing
A technology of oil exploitation and production technology, which is applied in the field of fracturing forging production, can solve the problems of inability to balance performance and yield, and achieve the effect of improving hardness, good strength and strong practicability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032] Embodiment 1: a kind of production technology of parts for fracturing of oil exploitation equipment, comprises the following steps:
[0033] (1) Refining: the mass percentage is Cu: 1%, Mg: 2%, Sn: 0.5%, Zr: 0.1%, Re: 0.05%, Ni: 0.01%, Si: 0.1%, Zn: 0.2%, SiC particles: 5%, rare earth: 0.05%, TiB: 3%, Al 2 o 3 1%, the balance is Fe raw materials for mixing and refining;
[0034] (2) Forging: Raw materials are initially smelted in an electric arc furnace and pretreated for desulfurization, and then blowing and slag removal using converter process dephosphorization technology. After deep desulfurization in LF ladle refining furnace, RH furnace vacuum circulation is used for degassing, and continuous casting of round billets is formed. billet to enhance product strength; high-quality electroslag ingots are used as raw materials, and an 8,000-ton water hydraulic press is used for three-phase forging to ensure uniform composition and compact structure of the forged bille...
Embodiment 2
[0057] Embodiment 2, a production process of parts and components for fracturing of oil extraction equipment, the refining step is: the mass percentage is Cu: 6%, Mg: 3%, Sn: 5%, Zr: 0.5%, Re : 2%, Ni: 0.5%, Si: 0.1%, Zn: 0.2%, SiC particles: 15%, rare earth: 0.2%, TiB: 8%, Al 2 o 3 : 2%, the balance is Fe raw materials for mixing and refining.
[0058] Other method steps in this embodiment are the same as in Embodiment 1.
Embodiment 3
[0059] Embodiment 3, a production process of components for fracturing of oil extraction equipment, the refining step is: the mass percentage is Cu: 3%, Mg: 5%, Sn: 3%, Zr: 0.3%, Re : 5%, Ni: 0.3%, Si: 0.3%, Zn: 0.4%, SiC particles: 10%, rare earth: 0.1%, TiB: 5%, Al 2 o 3 3%, and the balance is Fe for mixing and refining.
[0060] Other method steps in this embodiment are the same as in Embodiment 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com