Beneficiation method of copper-containing talc-serpentinite ore easy to argillate and float
A beneficiation method and serpentine technology, which are applied in the beneficiation of copper sulfide minerals, easy argillization, and easy-to-float copper-bearing talc-serpentine ores in the field of beneficiation, and can solve the problem of poor water solubility, easy-to-float talc-serpentine effects Problems such as flotation effect and difficulty in preparation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] Embodiment 1: as figure 1 with figure 2 Shown, a kind of beneficiation method of easily muddy, easily float copper-containing talc-serpentinite ore, carry out according to the following steps:
[0028] (1) Grinding: Grinding the ore that is easy to muddy and float with copper-containing talc-serpentinite, the grinding fineness is -0.074mm and the particle size content is 75%, so as to obtain the raw ore slurry;
[0029] (2) Pre-deliming flotation: add foaming agent butyl ether alcohol to the raw ore pulp, the dosage is 2g / t, and carry out pre-flotation of muddy and easy-to-float gangue, so as to obtain pre-deliming foam and pre-deliming pulp ;
[0030] (3) Separate flotation with pre-delimed foam: Add copper mineral inhibitors to the pre-delimed foam obtained in step (2), stir for 5 minutes, and perform desliming and reverse flotation to obtain reverse flotation mud foam and copper gangue-containing pulp after desliming, and reverse flotation desliming Foam is the...
Embodiment 2
[0037] Embodiment 2: as figure 1 with figure 2 Shown, a kind of beneficiation method of easily muddy, easily float copper-containing talc-serpentinite ore, carry out according to the following steps:
[0038] (1) Grinding: Grinding the ore that is easy to muddy and float with copper-containing talc-serpentinite, the grinding fineness is -0.074mm and the particle size content is 75%, so as to obtain the raw ore slurry;
[0039](2) Pre-deliming flotation: add foaming agent butyl ether alcohol to the raw ore pulp, the dosage is 2g / t, and carry out pre-flotation of muddy and easy-to-float gangue, so as to obtain pre-deliming foam and pre-deliming pulp ;
[0040] (3) Separate flotation with pre-delimed foam: Add copper mineral inhibitors to the pre-delimed foam obtained in step (2), stir for 5 minutes, and perform desliming and reverse flotation to obtain reverse flotation mud foam and copper gangue-containing pulp after desliming, and reverse flotation desliming Foam is the ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com