A technology of glass fiber and rare earth solution, which is applied in wood treatment, wood treatment details, reed/straw treatment, etc. It can solve the problems of limiting the application range of bamboo powder, prone to decay, mildew and insects, and shortening the service life of bamboo materials. , to achieve the effect of improving mildew and anticorrosion effects, improving mildew and anti-blue stain performance, and improving interface bonding performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] A method for treating bamboo with rare earth solution-glass fiber composite modification, is characterized in that it comprises the following steps:
[0028] (1) Pretreatment of bamboo:
[0029] Make a solution of 0.22 parts of silane coupling agent KH550 and absolute ethanol at a mass ratio of 1:5, then add 5 parts of nano-silica and 6 parts of chitosan, mix well, then evenly spray on the bamboo sample, and let it dry naturally ;
[0030] (2) Construction of interpenetrating polymers in bamboo:
[0031] Put the pretreated bamboo obtained in (1) in a vacuum drying dish, treat it under 0.1 MPa vacuum for 30 minutes, inhale the cross-linked polymer treatment solution, leave it for 2 hours, take it out, dry it at 80-85°C to constant weight, and then Heat up to 100-105°C and dry to absolute dryness;
[0032] (3) Plasticization modification process:
[0033] Soak the bamboo obtained in (2) in the plasticizer, put it in the treatment tank, keep it vacuumed for 10 minutes,...
Embodiment 2
[0042] A method for treating bamboo with rare earth solution-glass fiber composite modification, is characterized in that it comprises the following steps:
[0043] (1) Pretreatment of bamboo:
[0044] Make a solution of 0.38 parts of silane coupling agent KH550 and absolute ethanol at a mass ratio of 1:5, then add 9 parts of nano-silica and 10 parts of chitosan, mix well, then evenly spray on the bamboo sample, and let it dry naturally ;
[0045] (2) Construction of interpenetrating polymers in bamboo:
[0046] Put the pretreated bamboo obtained in (1) in a vacuum drying dish, treat it under 0.1MPa vacuum for 40 minutes, inhale the cross-linked polymer treatment solution, leave it for 3 hours, take it out, dry it at 85°C to constant weight, and then heat it up to Bake at 105°C until absolutely dry;
[0047] (3) Plasticization modification process:
[0048]Soak the bamboo obtained in (2) in the plasticizer, put it in the treatment tank, keep it vacuumed for 20 minutes, the...
PUM
Property | Measurement | Unit |
---|---|---|
friction coefficient | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com