Acetylated polyester modified electroconductive film and preparation method thereof
A technology of acetylated polyester and conductive film, applied in the field of solar cells, can solve the problems of low resistivity, poor toughness, poor compatibility, etc., to improve durability and reliability, improve dispersion compatibility, and improve mechanical properties Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A kind of acetylated polyester modified conductive film, it is made up of the raw material of following weight part:
[0022] Acetic anhydride 3, catalyst 0.01, methyl methacrylate 30, butyl acrylate 10, ammonium persulfate 1, polyphenylene ether 170, alkanolamide 1, 8-hydroxyquinoline 0.4, silane coupling agent kh550 2, light Quality calcium carbonate 10, solvent 300.
[0023] Described catalyzer is the sulfuric acid that concentration is 96%.
[0024] Described solvent is dimethylformamide.
[0025] A preparation method of acetylated polyester modified conductive film, comprising the following steps:
[0026] (1) Take ammonium persulfate, add it to deionized water 20 times its weight, and stir evenly;
[0027] (2) Take 8-hydroxyquinoline, add it to 7 times its weight in absolute ethanol, stir evenly, raise the temperature to 60°C, keep stirring for 10 minutes, add silane coupling agent kh550, and ultrasonicate for 3 minutes to obtain silane Alcoholic solution;
...
Embodiment 2
[0034] A kind of acetylated polyester modified conductive film, it is made up of the raw material of following weight part:
[0035] Acetic anhydride 4, catalyst 0.02, methyl methacrylate 40, butyl acrylate 15, ammonium persulfate 2, polyphenylene ether 200, alkanolamide 2, 8-hydroxyquinoline 1, silane coupling agent kh550 3, light Quality calcium carbonate 13, solvent 400.
[0036] The catalyst is sulfuric acid with a concentration of 96-98%.
[0037] Described solvent is dimethylformamide.
[0038] A preparation method of acetylated polyester modified conductive film, comprising the following steps:
[0039] (1) Take ammonium persulfate, add it to deionized water 30 times its weight, and stir evenly;
[0040] (2) Take 8-hydroxyquinoline, add it to 9 times its weight in absolute ethanol, stir evenly, raise the temperature to 65°C, keep stirring for 40 minutes, add silane coupling agent kh550, and ultrasonicate for 4 minutes to obtain silane Alcoholic solution;
[0041] (...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.