Ecological environment-friendly foaming lightweight wallboard and preparation method thereof
A light-weight wallboard and environment-friendly technology, applied to flat products, other household appliances, paints containing biocides, etc., can solve the problems of uneven surface, high cost, single appearance color, etc., and achieve good sound insulation effect and high quality Lightweight and cost-reducing effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0028] A method for preparing an eco-friendly foamed lightweight wallboard, the specific steps are:
[0029] Step 1. Pretreatment of raw materials: put wood powder and polyethylene particles into a dryer and dry them for later use; dissolve the silane coupling agent in ethanol solution to prepare a silane coupling agent solution with a mass fraction of 8%~10% For standby, after the glass fiber is burned and decontaminated, it is immersed in the prepared silane coupling agent solution for surface treatment, soaked for 30-60 minutes, and then transferred to a dryer for drying;
[0030] Step 2. Reinforcement of polyethylene particles: mill the dried glass fiber and polyethylene particles in the mill, adjust the roll distance of the mill, add polyethylene particles at 160~180°C, and cool to 130~145 ℃, add the dried glass fiber in batches and thin it out, repeat 3~5 times and cool naturally to get glass fiber modified polyethylene;
[0031] Step 3. Mixing materials: Add the glass ...
Embodiment 1
[0037] A method for preparing an eco-friendly foamed lightweight wallboard, the specific steps are:
[0038] Step 1, raw material pretreatment: according to the mass fraction, take 25 parts of 325-mesh wood powder and 39 parts of polyethylene regenerated particles and put them into the dryer for drying; 5 parts of KH550 are dissolved in ethanol solution to prepare the mass fraction of 8% KH550 solution for standby, after burning and decontaminating 8 parts of chopped glass fibers, immerse in the prepared KH550 solution for surface treatment, soak for 30min and then transfer to the dryer for drying;
[0039] Step 2. Reinforcement of polyethylene particles: Mill the dried glass fiber and polyethylene particles in the mill, adjust the roller distance of the mill, add polyethylene particles at 160°C, and cool them down to 130°C. Add dried glass fibers in batches and pass through, repeat 3 times and then cool naturally to obtain glass fiber modified polyethylene;
[0040] Step 3, mi...
Embodiment 2
[0046] A method for preparing an eco-friendly foamed lightweight wallboard, the specific steps are:
[0047] Step 1. Raw material pretreatment: According to the mass fraction, take 33.5 parts of 400-mesh wood flour and 48 parts of high-density polyethylene particles and put them in a dryer for drying; 2 parts of KH570 are dissolved in ethanol solution to prepare the mass fraction For 10% KH570 solution for use, 5 parts of chopped glass fibers are burned and decontaminated, then immersed in the prepared KH570 solution for surface treatment, soaked for 45 minutes, then transferred to a dryer for drying;
[0048] Step 2. Reinforcement of polyethylene particles: Mill the dried glass fiber and polyethylene particles in the mill, adjust the roller distance of the mill, add polyethylene particles at 170°C, and cool down to 140°C, Add dried glass fiber in batches and thin it out, repeat 4 times and then cool naturally to obtain glass fiber modified polyethylene;
[0049] Step 3, mixi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com