Anti-static down feather composite fibers for down and feather filled products
A down composite fiber and anti-static technology, which is applied in the field of anti-static down composite fiber for down products processing, can solve the problems of premature onset, aggravation of disease, bronchitis and asthma, etc., achieve excellent anti-static performance and enhance user comfort Sex, avoid static electricity effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0028] (1) Feather pretreatment: immerse the selected feathers in the cleaning agent, remove them after 10 minutes, and then rinse them with clean water to remove the dust and impurities attached to the feathers;
[0029] (2) Feather powder preparation: add water to 25g of feathers after pretreatment to adjust its water content at 65-70%, then add 3g of pregelatinized starch, mix well and send it to a freeze dryer, and dry the resulting solid through ultramicro The pulverizer makes fine powder, and then it is ground into nano-scale powder by nano ball mill, that is, feather powder;
[0030] (3) Preparation of silky down fiber: add 70g 5wt% peracetic acid solution to the 25g feather powder of the above-mentioned gained, fully mix and soak for 24h, and microwave reflux treatment at microwave frequency 2450MHz, output power 700W for 10min, filter while hot, The obtained filtrate was naturally cooled to room temperature, and then the pH value of the filtrate was adjusted to 7 with...
Embodiment 2
[0037] (1) Feather pretreatment: immerse the selected feathers in the cleaning agent, remove them after 10 minutes, and then rinse them with clean water to remove the dust and impurities attached to the feathers;
[0038] (2) Feather meal preparation: add water to 30g of feathers after pretreatment to adjust its water content at 65-70%, then add 3g of pregelatinized starch, mix well and send it to a freeze dryer, and dry the resulting solid through ultramicro The pulverizer makes fine powder, and then it is ground into nano-scale powder by nano ball mill, that is, feather powder;
[0039] (3) Preparation of filamentous down fiber: add 80g 5wt% peracetic acid solution to the above-mentioned gained 30g feather powder, soak for 24h after fully mixing, and process 10min under microwave reflux at microwave frequency 2450MHz, output power 700W, filter while hot, The obtained filtrate was naturally cooled to room temperature, and then the pH value of the filtrate was adjusted to 7 by...
Embodiment 3
[0072] Taking the same batch of feathers as raw materials, the down composite fibers were prepared by the methods of Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 3 respectively, and the comparative example 4 without modification treatment was set at the same time, and the determination The method is used to remove dust and impurities on feathers in the feather pretreatment stage, and measure the antistatic performance of the prepared down composite fiber. The results are shown in Table 1.
[0073] The application performance of down composite fiber preparation method described in table 1 embodiment and comparative example
[0074]
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com