An anti-rust coating, marine technology, applied in anti-corrosion coatings, anti-fouling/underwater coatings, coatings, etc., can solve the problems of clogging pipes and breeding nets, loss, accelerated metal corrosion, etc., to achieve strong inhibition of adhesion, The effect of reducing friction coefficient and improving water repellency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] An environment-friendly biomimetic marine anti-rust paint is characterized in that it is made of the following raw materials in parts by weight:
[0016] 20 parts of fluorinated acrylate, 22 parts of epoxy phenolic resin, 12 parts of silicone rubber, 10 parts of silicon aluminum barium calcium alloy powder, 3 parts of titanium dioxide, 2 parts of biological preservative, 3 parts of adhesion thickener, 5 parts of filler Parts, 24 parts of solvent.
[0017] Further, the solvent is a mixture of propylene glycol and polytetrafluoroethylene in a weight ratio of 3:1.
[0018] Further, the adhesion thickener is a mixture of modified hydrogenated castor oil and hydroxyethyl cellulose in a weight ratio of 1:3.
[0019] Further, the filler is a mixture of kaolin and mica powder in a weight ratio of 1:1.
[0020] Further, the biological preservative is a mixture of sodium benzoate, gingerol, and P-cinnamic acid sulfate in a weight ratio of 1:1:2.
Embodiment 2
[0022] An environment-friendly biomimetic marine anti-rust paint is characterized in that it is made of the following raw materials in parts by weight:
[0023] 23 parts of fluorinated acrylate, 23 parts of epoxy phenolic resin, 13 parts of silicone rubber, 11 parts of silicon aluminum barium calcium alloy powder, 3.5 parts of titanium dioxide, 3 parts of biological preservative, 3.5 parts of adhesion thickener, 6 parts of filler Parts, 26 parts of solvent.
[0024] Further, the solvent is a mixture of propylene glycol and polytetrafluoroethylene in a weight ratio of 3:1.
[0025] Further, the adhesion thickener is a mixture of modified hydrogenated castor oil and hydroxyethyl cellulose in a weight ratio of 1:3.
[0026] Further, the filler is a mixture of kaolin and mica powder in a weight ratio of 1:1.
[0027] Further, the biological preservative is a mixture of sodium benzoate, gingerol, and P-cinnamic acid sulfate in a weight ratio of 1:1:2.
Embodiment 3
[0029] An environment-friendly biomimetic marine anti-rust paint is characterized in that it is made of the following raw materials in parts by weight:
[0030] 25 parts of fluorinated acrylate, 24 parts of epoxy phenolic resin, 15 parts of silicone rubber, 12 parts of silicon aluminum barium calcium alloy powder, 4 parts of titanium dioxide, 4 parts of biological preservative, 4 parts of adhesion thickener, 7 parts of filler Parts, 28 parts of solvent.
[0031] Further, the solvent is a mixture of propylene glycol and polytetrafluoroethylene in a weight ratio of 3:1.
[0032] Further, the adhesion thickener is a mixture of modified hydrogenated castor oil and hydroxyethyl cellulose in a weight ratio of 1:3.
[0033] Further, the filler is a mixture of kaolin and mica powder in a weight ratio of 1:1.
[0034] Further, the biological preservative is a mixture of sodium benzoate, gingerol, and P-cinnamic acid sulfate in a weight ratio of 1:1:2.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com