Plastic for flame-retardant, wear-resistant and aging-resistant mobile telephone shell
A mobile phone casing and anti-aging technology, which is applied in the field of plastics for flame-retardant, wear-resistant and anti-aging mobile phone casings, can solve the problems of shortened life of plastic mobile phone casings, poor wear resistance, aging resistance, and poor flame retardant performance, and achieves a remarkable concealing effect. , Good waterproof and flame retardant properties, and the effect of enhancing mechanical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A flame-retardant, wear-resistant and aging-resistant plastic for mobile phone casings, the raw materials of which include by weight: 10 parts of polycarbonate, 18 parts of polypropylene, 20 parts of ethylene-octene copolymer, 25 parts of polyvinyl chloride, maleic anhydride Branch ethylene-vinyl acetate copolymer 8 parts, silicon carbide 8 parts, silane coupling agent SI-691 parts, alumina 4 parts, iron-based montmorillonite 2 parts, boron nitride 3 parts, nano silicon dioxide 8 parts, 16 parts of modified opal powder, 8 parts of calcined kaolin, 3 parts of phenylene bismaleimide, 1 part of natural rubber grafted polymethyl methacrylate, 3 parts of caprolactam, 1 part of benzoyl peroxide, Sanya 0.6 parts of ethyltetramine, 0.2 parts of cyclohexanone peroxide, 2 parts of tert-butyl perbenzoate, 1 part of dioctadecyl ester, 3 parts of p-phenylenediamine, and 1 part of trioctyl ester.
Embodiment 2
[0018] A flame-retardant, wear-resistant and aging-resistant plastic for mobile phone casings, the raw materials of which include by weight: 18 parts of polycarbonate, 5 parts of polypropylene, 40 parts of ethylene-octene copolymer, 15 parts of polyvinyl chloride, maleic anhydride Branched ethylene-vinyl acetate copolymer 16 parts, silicon carbide 2 parts, silane coupling agent SI-692.5 parts, alumina 1 part, iron-based montmorillonite 10 parts, boron nitride 1 part, nano silicon dioxide 12 parts, 5 parts of modified opal powder, 14 parts of calcined kaolin, 1 part of phenylene bismaleimide, 3 parts of natural rubber grafted polymethyl methacrylate, 1 part of caprolactam, 2 parts of benzoyl peroxide, Sanya 0.2 parts of ethyl tetramine, 0.6 parts of cyclohexanone peroxide, 1 part of tert-butyl perbenzoate, 3 parts of dioctadecyl ester, 1 part of p-phenylenediamine, and 3 parts of trioctyl ester.
Embodiment 3
[0020] A flame-retardant, wear-resistant and aging-resistant plastic for mobile phone casings, the raw materials of which include by weight: 14 parts of polycarbonate, 15 parts of polypropylene, 30 parts of ethylene-octene copolymer, 24 parts of polyvinyl chloride, maleic anhydride 12 parts of branched ethylene-vinyl acetate copolymer, 6 parts of silicon carbide, 1.5 parts of silane coupling agent SI-69, 2.8 parts of alumina, 3 parts of iron-based montmorillonite, 2.8 parts of boron nitride, 9 parts of nano-silica, 12 parts of modified opal powder, 11 parts of calcined kaolin, 2.5 parts of phenylene bismaleimide, 2 parts of natural rubber grafted polymethyl methacrylate, 2 parts of caprolactam, 1.6 parts of benzoyl peroxide, Sanya 0.5 parts of ethyl tetramine, 0.4 parts of cyclohexanone peroxide, 1.6 parts of tert-butyl perbenzoate, 1.5 parts of dioctadecyl ester, 2 parts of p-phenylenediamine, and 1.5 parts of trioctyl ester.
[0021] The modified opal powder is prepared by t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com