Preparation method of flame-retardant antistatic plastic liner plate
A flame-retardant, anti-static, plastic technology, applied in the field of plastic materials, can solve the problems of long downtime, short service life, easy wear, etc., and achieve the effects of good moisture resistance, good anti-static performance and long service life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0013] A method for preparing a flame-retardant antistatic plastic liner, comprising the following steps:
[0014] 1) Take the following raw materials in parts by weight: 100 parts of polypropylene, 40-80 parts of high-density polyethylene, 20-30 parts of glass fiber, 15-20 parts of glass microspheres, 5-15 parts of talcum powder, 5 parts of calcium carbonate ~15 parts, 0.5~1.5 parts of silane coupling agent, 10~15 parts of POE, 1~3 parts of sodium dodecylsulfonate, 5~10 parts of decabromodiphenylethane, 10~15 parts of conductive carbon black, 0.5-1.5 parts of oxygen agent and 5-10 parts of dioctyl phthalate, set aside;
[0015] Described antioxidant is antioxidant 1010.
[0016] The weight-average molecular weight of the high-density polyethylene is 200,000-350,000.
[0017] 2) Put the glass fiber, glass microspheres, talcum powder, calcium carbonate, silane coupling agent and dioctyl phthalate obtained in step 1) into a high-speed mixer, and stir at 40-60°C 10min, then ad...
Embodiment 1
[0021] A method for preparing a flame-retardant antistatic plastic liner, comprising the following steps:
[0022] 1) Take the following raw materials in parts by weight: 100 parts of polypropylene, 40 parts of high-density polyethylene, 30 parts of glass fiber, 15 parts of glass microspheres, 5 parts of talcum powder, 15 parts of calcium carbonate, and 0.5 parts of silane coupling agent , 15 parts of POE, 1 part of sodium dodecyl sulfonate, 10 parts of decabromodiphenylethane, 10 parts of conductive carbon black, 1.5 parts of antioxidant (1010) and 5 parts of dioctyl phthalate, set aside;
[0023] The weight-average molecular weight of the high-density polyethylene is 200,000-350,000.
[0024] 2) Put the glass fiber, glass microspheres, talcum powder, calcium carbonate, silane coupling agent and dioctyl phthalate obtained in step 1) into a high-speed mixer, and stir for 10 minutes at 40°C. Then add decabromodiphenylethane, sodium dodecyl sulfonate, conductive carbon blac...
Embodiment 2
[0034] A method for preparing a flame-retardant antistatic plastic liner, comprising the following steps:
[0035] 1) Take the following raw materials in parts by weight: 100 parts of polypropylene, 80 parts of high-density polyethylene, 20 parts of glass fiber, 20 parts of glass microspheres, 15 parts of talcum powder, 5 parts of calcium carbonate, and 1.5 parts of silane coupling agent , 10 parts of POE, 3 parts of sodium dodecyl sulfonate, 5 parts of decabromodiphenylethane, 15 parts of conductive carbon black, 0.5 parts of antioxidant (1010) and 10 parts of dioctyl phthalate, set aside;
[0036] The weight-average molecular weight of the high-density polyethylene is 200,000-350,000.
[0037] 2) Put the glass fiber, glass microspheres, talcum powder, calcium carbonate, silane coupling agent and dioctyl phthalate obtained in step 1) into a high-speed mixer, and stir for 10 minutes at 60°C. Then add decabromodiphenylethane, sodium dodecyl sulfonate, conductive carbon bla...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology