Colored dust-free chalk capable of fading automatically and preparation method thereof
A color and automatic technology, applied in the field of chalk for teaching and its preparation, can solve the problems that handwriting cannot be automatically faded, the user's health is unfavorable, the molecular binding force is weak, etc., and the effect of smooth writing, not easy to fall off, and bright colors can be achieved.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0009] Embodiment 1: prepare red chalk
[0010] Components: sodium thiosulfate 8g, sodium carbonate 0.352g, phenolphthalein 1.28g, talcum powder 0.5g, carboxymethylcellulose sodium 0.1g, sodium metasilicate nonahydrate 2g.
[0011] Preparation method: mix phenolphthalein and sodium carbonate, add absolute ethanol dropwise to a thick paste, pour molten sodium thiosulfate and sodium metasilicate nonahydrate into it and stir evenly, then add talcum powder and carboxymethyl cellulose Sodium and stir evenly, pour into the mold, dry in the air, take it out, soak it with 10% polyvinylpyrrolidone absolute ethanol solution for one minute and cover the film, take it out and dry it.
[0012] Effect: The chalk has high chroma, good coverage, moderate softness and hardness, and can withstand a temperature of 45°C. The handwriting fades in 2 hours in rainy weather and 2 days in dry weather.
Embodiment 2
[0013] Embodiment 2: prepare yellow chalk
[0014] Components: sodium thiosulfate 8g, sodium carbonate 0.368g, m-nitrophenol 1.28g, talcum powder 1g, sodium carboxymethylcellulose 0.1g, sodium metasilicate nonahydrate 1.8g.
[0015] Preparation method: mix m-nitrophenol and sodium carbonate, add absolute ethanol dropwise to a thick paste, pour molten sodium thiosulfate and sodium metasilicate nonahydrate into it and stir evenly, then add talc powder and carboxymethyl Base cellulose sodium and stir evenly, pour into the mold, dry, soak with 10% polyvinylpyrrolidone absolute ethanol solution for one minute and cover the film after taking it out, take it out and dry it.
[0016] Effect: The chalk has high chroma, good coverage, moderate softness and hardness, and can withstand a temperature of 45°C. The handwriting fades in 2 hours in rainy weather and 2 days in dry weather.
Embodiment 3
[0017] Embodiment 3: prepare orange chalk
[0018] Components: 8g of sodium thiosulfate, 0.355g of sodium carbonate, 0.7g of phenolphthalein, 0.66g of m-nitrophenol, 1g of talc, 0.1g of sodium carboxymethylcellulose, and 1.5g of sodium metasilicate nonahydrate.
[0019] Preparation method: mix phenolphthalein, m-nitrophenol and sodium carbonate, add absolute ethanol dropwise to adjust to a thick paste, pour molten sodium thiosulfate and sodium metasilicate nonahydrate into it and stir evenly, add talcum powder and Sodium carboxymethyl cellulose and stir evenly, pour into the mould, dry, soak with 10% polyvinylpyrrolidone absolute ethanol solution for one minute and cover the film after taking it out, take it out and dry it.
[0020] Effect: The chalk has high chroma, good coverage, moderate softness and hardness, and can withstand a temperature of 45°C. The handwriting fades in 2 hours in rainy weather and 2 days in dry weather.
PUM
Property | Measurement | Unit |
---|---|---|
thermal resistance | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com