Method for simultaneously preparing pyromellitic acid and terephthalic acid with coal serving as raw material
A technology of pyromellitic acid and terephthalic acid, applied in chemical instruments and methods, preparation of carboxylic acid by ozone oxidation, preparation of carboxylate, etc. Social and economic benefits, the effect of broad application prospects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The anthracite is crushed, shrunk and ground to 40 mesh according to the national standard, and the temperature is about 80 ℃, the vacuum degree is 10 -2 Bake at mmHg until the moisture is less than 1.0% as the oxidation test sample.
[0026] The equipment used in the experiment is the GSHA-1.5L autoclave produced by Shandong Penglai Luhao Chemical Machinery Co., Ltd. Oxidation test The weight of the anthracite coal put into the kettle is 10g, potassium hydroxide 50g, distilled water 180g, filled with O 2 To 6.0MPa, rise to 360°C under stirring, stop heating after constant temperature oxidation for 1h. After cooling, the oxidation product is removed from the autoclave and the insoluble residue (slag + minerals) is filtered off. The filtrate was acidified with concentrated sulfuric acid to pH=3, and then the humic acid was filtered off, and the filtrate was acidified with concentrated sulfuric acid to pH=1.5. Then the filtrate was extracted several times with butanone...
Embodiment 2
[0031] Aged bituminous coal is crushed, shrunk and ground to 80 meshes according to national standards, and is heated at a temperature of about 80°C and a vacuum of 10 -2 Bake at mmHg until the moisture is less than 1.0% as the oxidation test sample.
[0032] The equipment used in the experiment is the GSHA-1.5L autoclave produced by Shandong Penglai Luhao Chemical Machinery Co., Ltd. Oxidation test The weight of old bituminous coal put into the kettle is 20g, the mixture of calcium hydroxide and sodium methoxide is 200g, distilled water is 2.2g, filled with O 2 To 1MPa, rise to 100°C under stirring, stop heating after constant temperature oxidation for 0.5h. After cooling, the oxidation product is removed from the autoclave and the insoluble residue (slag + minerals) is filtered off. The filtrate was acidified with concentrated sulfuric acid to pH=2, and then humic acid was filtered out, and the filtrate was acidified with concentrated sulfuric acid to pH=1. Then the filtr...
Embodiment 3
[0037] The mixture of anthracite and aged bituminous coal is crushed, shrunk and ground to 60 meshes according to national standards, and is heated at a temperature of about 80°C and a vacuum of 10 -2 Bake at mmHg until the moisture is less than 1.0% as the oxidation test sample.
[0038] The equipment used in the experiment is the GSHA-1.5L autoclave produced by Shandong Penglai Luhao Chemical Machinery Co., Ltd. Alkali Oxygen Oxidation Test 100g of anthracite and aged bituminous coal mixture, 10g of ammonia water, 200g of distilled water, O 2 Pressurize to 10MPa, rise to 400°C under stirring, stop heating after constant temperature oxidation for 5h. After cooling, the oxidation product is removed from the autoclave and the insoluble residue (slag + minerals) is filtered off. The filtrate was acidified with concentrated sulfuric acid to pH=5, and then humic acid was filtered out, and the filtrate was acidified with concentrated sulfuric acid to pH=3. Then the filtrate was ...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com