Tape base paper and production method thereof

A production method and adhesive tape technology, applied in paper, papermaking, paper machines, etc., can solve the problems of affecting product performance, high production cost, high beating degree, etc., achieve the effect of reducing beating degree, guaranteed source, and improving kappa value

Inactive Publication Date: 2011-05-04
YONGZHOU XIANGJIANG PAPER CO LTD
View PDF2 Cites 7 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, the tape base paper production method disclosed in the patent application documents all uses coniferous wood pulp, and the production cost is high; the amount of PAE-LT wet strength agent is as high as 5-10% (for absolute dry pulp, the amount of wet strength agent is calculated as 100%), The production cost is high, and the broken paper produced in the papermaking process is difficult to handle due to high wet strength, which limits the use of this production method; the use of viscous beating method, high beating degree, not only causes high energy consumption, but also affects the performance of the product

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0017] With 60 parts by weight of masson pine, 20 parts by weight of hardwood, and 20 parts by weight of Chinese fir side boards, after preparing materials, adopt low-energy consumption displacement cooking, closed washing and sieving to make chemical natural color wood pulp with a kappa value of 40, pulp After oxygen-alkali delignification and hydrogen peroxide bleaching, the pulp whiteness is at 19% (ISO), and this slurry is blended into a concentration of 3.4%, the slurry is beaten to 27 ° SR, wet weight 12g, and the slurry is passed through Remove sand after dilution, control the online concentration of 0.25%, the online pH value: 6.5, pass through the pressure sieve and fine screen, use the PEA wet strength agent seasoning with a dry weight ratio of 1% to the pulp, fourdrinier paper machine forming, pressing, drying, Coiling, rewinding, packaging into finished products.

[0018] Oxygen delignification hydrogen peroxide bleaching process is oxygen delignification period of...

Embodiment 2

[0021] With 50 parts by weight of masson pine, 30 parts by weight of hardwood, and 25 parts by weight of fir edge boards, after preparing materials, adopt DDS displacement cooking, closed washing and sieving to make chemical natural wood pulp with a Kappa value of 50. Oxygen-alkali delignification, hydrogen peroxide bleaching pulp whiteness at 26% (ISO), this slurry is adjusted to a concentration of 3.0%, the slurry is beaten to 29 ° SR, wet weight 12.3g, the slurry is passed through Remove sand after dilution, control the concentration of 0.22% on the net, the pH value of the net: 6.1, pass through the pressure sieve and fine screen, use the PEA wet strength agent seasoning with a dry weight ratio of 4% of the pulp, fourdrinier paper machine forming, pressing, extensibility Compression, drying, coiling, rewinding, packaging into finished products.

[0022] Oxygen delignification hydrogen peroxide chlorine-free bleaching process is oxygen delignification period time 80 minutes...

Embodiment 3

[0025] With 55 parts by weight of masson pine, 25 parts by weight of broad-leaved wood, 10 parts by weight of fir side boards, and 10 parts by weight of plywood processing residues, after preparing materials, adopt DDS displacement cooking, closed washing and sieving to make kappa value 42 Chemical uncolored wood pulp, the pulp whiteness is 27% (ISO) after oxygen-alkali delignification and hydrogen peroxide bleaching, the pulp is blended into a concentration of 4.4%, the pulp is beaten to 32 ° SR, wet The weight is 14g. After the slurry is diluted, the sand is removed. The online concentration is controlled to 0.2%. Forming, pressing, stretching compression, drying, coiling, rewinding, packaging into finished products.

[0026] Oxygen delignification hydrogen peroxide chlorine-free bleaching process is oxygen delignification period of 90 minutes, pulp concentration 12%, temperature 100 ℃, oxygen pressure 1050Kpa, pH value 11.5, oxygen consumption per ton of air-dried pulp 30kg...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
Tensile strengthaaaaaaaaaa
Tightnessaaaaaaaaaa
Wet strengthaaaaaaaaaa
Login to view more

Abstract

The invention provides tape base paper and a production method thereof. As for the tap base paper, the fracture length is more than or equal to 6.0km; the tensile strength is more than or equal to 1.5kN / m; the moisture content is within the range of 7-10%; the tightness is more than or equal to 0.62g / cm<3>; the wet strength is more than or equal to 0.33kN / m; and the whiteness is within the range of 17-25%. The production method of the tape base paper comprises the following steps: carrying out low-energy consumption displacement cooking, oxygen-alkali delignification and hydrogen peroxide bleaching processes on a wood fiber raw material to produce micro-bleaching pulp, wherein the whiteness of the bleached pulp is 19-27%, the beating concentration of the bleached pulp is 2.5-4.5%, the beating degree of the bleached pulp is 26-32 degree SR, and the wet weight of the bleached pulp is 10.5-15g; and the pulp is formed by beating, degritting, adding a wet strength agent, carrying out fine screening with a pressurized screen, forming on a mesh, squeezing, drying, reeling, rewinding, and packaging.

Description

technical field [0001] The invention relates to an adhesive tape base paper, which has high dry and wet physical strength and brown color, and is suitable for producing adhesive tapes. The invention also relates to the production method of the tape base paper, especially the technology of using needle and broadwood fiber raw materials, adopting DDS low energy consumption displacement cooking, oxygen delignification and hydrogen peroxide bleaching process to produce the tape base paper. Background technique [0002] In the automotive, home improvement, packaging and other industries, a tape is used for blocking or bonding. At present, the tapes on the market mainly include plastic tapes and paper-based tapes. The paper sheets used to produce paper-based tapes are required to have certain physical strength, water resistance, and aging resistance, so as to ensure the normal production and tape products during the tape processing and production process. quality. To produce tap...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): D21H27/00D21F11/00D21H11/14D21H21/20
Inventor 王福纪朱杰刘便初赵桂林梁好新张素卫王敏潘贞叶张勇
Owner YONGZHOU XIANGJIANG PAPER CO LTD
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products