A hydrotreating and catalyst technology, applied in refining to remove heteroatoms, etc., can solve the problems that are not conducive to improving the catalytic activity and performance, affect the surface properties and performance of the carrier, and the inhomogeneity of the carrier properties. The effect of dispersion, easy molding, increasing pore volume and volume specific surface area
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] (1) Preparation of phosphorus-containing aluminum hydroxide
[0029] Add 2500ml of deionized water into a clean container, heat up to 65°C, and under stirring conditions, add an aqueous solution of aluminum sulfate with a specific gravity of 1.14 and an aqueous solution of sodium metaaluminate with a specific gravity of 1.37 to the stirred deionized water at the same time, and keep The temperature was 65°C, the pH was 8.5, and the addition time was 75 minutes. After stopping feeding, age for 60 minutes, add deionized water to the filtered filter cake, and wash the material 4 times to make the Na in the material + Content4 2- Content3+ content <0.08m%, then add the filtered aluminum hydroxide filter cake to a solution of 2.0L deionized water and 45g 85m% phosphoric acid to make a slurry evenly, control the temperature of the slurry at 85°C, and filter the filter cake directly after slurrying for 40 minutes After drying at 110°C for 8 hours, it was pulverized for use. ...
Embodiment 2
[0037] In embodiment 1, the add-on of 85m% phosphoric acid is changed into 58g by 45g, and the charging amount of each other material and operating condition are all identical with embodiment 1, promptly cost example.
Embodiment 3
[0039] In embodiment 1, the add-on of 85m% phosphoric acid is changed into 70g by 45g, the half that nano silicon-containing compound is used adds after wetting with the nitric acid aqueous solution of 30ml 2.5%, half adds by embodiment 1 adding method, and material Kneading, the feeding amount and operating conditions of other materials are all the same as in Example 1, which is a cost example.
PUM
Property | Measurement | Unit |
---|---|---|
specific surface area | aaaaa | aaaaa |
specific surface area | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com