Production formula of gold wavy inter-chip and production process of production formula
A technology for producing formula and gold, which is applied in the field of pure gold, which can solve the problems of poor color gloss, easy falling off of structure, and loose connection, etc., and achieve the effect of long color retention time, reducing the link of frying acid, and facilitating welding and forming
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] In the embodiment of the present invention, a production formula of a gold water-wave inter-sheet is prepared from the following raw materials in parts by weight: 99.92 parts of gold, 0.08 parts of alloy metal, and the metal alloy includes copper, silver, sodium and trace metal elements, Among them, 0.0384 parts of copper, 0.0184 parts of silver, 0.008 parts of sodium and 0.0152 parts of trace metal elements.
Embodiment 2
[0030] In the embodiment of the present invention, a production formula of a gold water-wave inter-sheet is prepared from the following raw materials in parts by weight: 99.95 parts of gold, 0.05 parts of alloy metal, and the metal alloy includes copper, silver, sodium and trace metal elements, Among them, 0.024 parts of copper, 0.0115 parts of silver, 0.005 parts of sodium and 0.0095 parts of trace metal elements.
Embodiment 3
[0032] In the embodiment of the present invention, a production formula of a gold water-wave inter-sheet is prepared by including the following raw materials in parts by weight: 99.97 parts of gold, 0.03 parts of alloy metal, and the metal alloy includes copper, silver, sodium and trace metal elements, Among them, 0.0144 parts of copper, 0.0069 parts of silver, 0.003 parts of sodium and 0.0057 parts of trace metal elements.
[0033] The technique of embodiment 1-3, comprises the following steps:
[0034] 1. The general department will distribute the high-purity gold raw materials and alloy metal particles according to the ratio and distribute them to the melting gold department. After melting, put alloy metal particles in proportion and stir for 2-3 minutes. The stirring tool is a quartz rod. The temperature of the gold melting furnace is within 1050-1080 degrees Celsius, and the time for melting gold is 5-10 minutes. You can take out the gold melting cylinder with tongs, pou...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com