Cast copper sculpture material and preparation process of cast copper sculpture
A preparation process and sculpture technology, applied in metal material coating process, superimposed layer plating, coating and other directions, can solve the problems of large manpower and financial resources, high cost of raw materials, and increased cost of cast copper sculpture.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The present invention proposes a cast copper sculpture material, comprising the following mass ratio components: 45 parts of metal copper, 30 parts of metal tin, 20 parts of metal aluminum, 30 parts of metal zinc, 15 parts of silicon, 30 parts of metal iron, 10 parts of metal nickel, 5 parts of chromium metal, 5 parts of graphite, 2 parts of titanium metal, 1-2 parts of magnesium metal and 2 parts of cullet.
[0026] The metal copper is heat-treated modified copper.
[0027] The heat treatment process of the metal copper is as follows: hot rolling the metal copper at a temperature of 625 degrees Celsius, and then performing a high-temperature annealing treatment at an environment of 320 degrees Celsius for 3 hours to obtain modified copper.
[0028] A preparation process for cast copper sculpture, comprising the following steps:
[0029] Step 1: Metal copper, metal tin, metal aluminum, metal zinc, metal iron, metal nickel, metal chromium, metal titanium and metal magne...
Embodiment 2
[0037] The present invention proposes a cast copper sculpture material, comprising the following mass ratio components: 48 parts of metal copper, 32 parts of metal tin, 23 parts of metal aluminum, 32 parts of metal zinc, 20 parts of silicon, 35 parts of metal iron, 11 parts of metal nickel, 6 parts of chromium metal, 6 parts of graphite, 3 parts of titanium metal, 1.5 parts of magnesium metal and 2.5 parts of cullet.
[0038] The metal copper is heat-treated modified copper.
[0039] The heat treatment process of the metal copper is as follows: hot rolling the metal copper at a temperature of 625 degrees Celsius, and then performing a high-temperature annealing treatment at an environment of 320 degrees Celsius for 3 hours to obtain modified copper.
[0040] A preparation process for cast copper sculpture, comprising the following steps:
[0041] Step 1: Metal copper, metal tin, metal aluminum, metal zinc, metal iron, metal nickel, metal chromium, metal titanium and metal mag...
Embodiment 3
[0049] The present invention proposes a cast copper sculpture material, comprising the following mass ratio components: 50 parts of metal copper, 35 parts of metal tin, 25 parts of metal aluminum, 35 parts of metal zinc, 25 parts of silicon, 40 parts of metal iron, 12 parts of metal nickel, 8 parts chrome metal, 8 parts graphite, 4 parts titanium metal, 2 parts magnesium metal and 3 parts cullet.
[0050] The metal copper is heat-treated modified copper.
[0051] The heat treatment process of the metal copper is as follows: hot rolling the metal copper at a temperature of 625 degrees Celsius, and then performing a high-temperature annealing treatment at an environment of 320 degrees Celsius for 3 hours to obtain modified copper.
[0052] A preparation process for cast copper sculpture, comprising the following steps:
[0053] Step 1: Metal copper, metal tin, metal aluminum, metal zinc, metal iron, metal nickel, metal chromium, metal titanium and metal magnesium are smelted se...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com