Preparation method of quickly degreased degreasant material for leather making
A degreaser and fast technology, applied in leather degreasing, application, small raw hide/large raw hide/leather/fur treatment, etc., can solve the problem of poor degreasing effect of leather degreaser, achieve fast and effective degreasing, good synergistic effect, improve The effect of degreasing rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0025] In parts by weight, weigh 45 to 50 parts of sodium dodecylbenzenesulfonate, 10 to 15 parts of polyacrylamide and 6 to 8 parts of sodium nonylphenol polyoxyethylene ether carboxylate, place them in a mixer, and stir Mix and collect the mixed solution, let it stand for defoaming for 6-8 hours, and obtain the composite surfactant material; in parts by weight, weigh 45-50 parts of deionized water, 3-5 parts of chitosan, 1-2 parts of Put glacial acetic acid and 6-8 parts of composite surfactants in a three-necked flask, stir and mix them, and ventilate the air with nitrogen. Control the rate of nitrogen gas introduction at 10-15mL / min. The mass ratio is 1:15, add the ammonium persulfate solution with a mass fraction of 15% dropwise to the mixed solution, and control the drop rate of the ammonium persulfate solution at a rate of 1-2mL / min. Insulate and react at 65°C for 1 to 2 hours to obtain the reaction solution and weigh 45 to 50 parts of the reaction solution, 10 to 15 pa...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.